MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lotte Advanced Materials Infino® AE-2150 PC/PET, 15% MF  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/PET Polyester Blend; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: General, automotive

Information provided by Lotte Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.33 g/cc1.33 g/ccNatural or representative color; ASTM D792
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm
@Thickness 3.20 mm
0.0040 - 0.0060 in/in
@Thickness 0.126 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
ASTM D955
Melt Flow 34 g/10 min
@Load 5.00 kg,
Temperature 260 °C
34 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
Ash 15 %15 %ASTM D5630
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 110110ASTM D785
Tensile Strength at Break 58.8 MPa8530 psi5 mm/min; ASTM D638
Tensile Strength, Yield 65.7 MPa9530 psi5 mm/min; ASTM D638
Elongation at Break 7.0 %7.0 %5 mm/min; ASTM D638
Tensile Modulus 3.53 GPa512 ksi5 mm/min; ASTM D638
Flexural Strength 86.3 MPa12500 psi2.8 mm/min; ASTM D790
Flexural Modulus 3.92 GPa569 ksi2.8 mm/min; ASTM D790
Izod Impact, Notched  0.490 J/cm
@Thickness 6.35 mm,
Temperature -30.0 °C
0.918 ft-lb/in
@Thickness 0.250 in,
Temperature -22.0 °F
ASTM D256
 0.490 J/cm
@Thickness 3.17 mm,
Temperature -30.0 °C
0.918 ft-lb/in
@Thickness 0.125 in,
Temperature -22.0 °F
ASTM D256
 0.588 J/cm
@Thickness 6.35 mm,
Temperature 23.0 °C
1.10 ft-lb/in
@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D256
 0.588 J/cm
@Thickness 3.17 mm,
Temperature 23.0 °C
1.10 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 46.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
25.6 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
CTE, linear, Transverse to Flow 66.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
36.7 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 130 °C
@Thickness 6.40 mm
266 °F
@Thickness 0.252 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 123 °C
@Thickness 6.40 mm
253 °F
@Thickness 0.252 in
ASTM D648
Vicat Softening Point 137 °C279 °FB/50; ISO R 306

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lotte Advanced Materials Infino® AE-2230 PC/PET, 20% MF
MRC Polymers NAXALOY™ 793 PC/PET Blend, High Impact Strength and Chemical Resistance
Covestro Makroblend® AR205 PC+PET
Lotte Advanced Materials Infino® AE-2030 PC/PET, General Purpose
Lotte Advanced Materials Infino® AE-2130 PC/PET, 5% MF

PLOTT9801 / 205664

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.