MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

MRC Polymers NAXALOY™ 793 PC/PET Blend, High Impact Strength and Chemical Resistance  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/PET Polyester Blend; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: PC/PET Blend, Weatherable, High Impact Strength and Chemical Resistance, Dimensional Stability

Mechanical properties measured on 1/8 in. (3.2 mm) samples.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.21 g/cc0.0437 lb/in³ASTM D792
Water Absorption 0.14 %0.14 %24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0080 cm/cm0.0050 - 0.0080 in/in1/8" (3.2 mm); ASTM D955
Linear Mold Shrinkage, Transverse 0.0070 - 0.0090 cm/cm0.0070 - 0.0090 in/inASTM D955
Melt Flow 18 g/10 min
@Load 2.16 kg,
Temperature 275 °C
18 g/10 min
@Load 4.76 lb,
Temperature 527 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 56.0 MPa8120 psiASTM D638
Elongation at Break 50 %50 %ASTM D638
Flexural Yield Strength 83.0 MPa12000 psiASTM D790
Flexural Modulus 2.136 GPa309.8 ksiASTM D790
Izod Impact, Notched 6.41 J/cm12.0 ft-lb/inASTM D256
Impact Test 44.0 J
@Temperature 23.0 °C
32.5 ft-lb
@Temperature 73.4 °F
ASTM D3763
 46.0 J
@Thickness 3.17 mm,
Temperature -30.0 °C
33.9 ft-lb
@Thickness 0.125 in,
Temperature -22.0 °F
46 J Instrumented Impact Total Energy; 7.5 MPH (12.23 km/h).; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear 61.2 µm/m-°C
@Temperature -40.0 - 35.0 °C
34.0 µin/in-°F
@Temperature -40.0 - 95.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 132 °C270 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 115 °C239 °FUnannealed; ASTM D648
Flammability, UL94 HB
@Thickness 1.47 mm
HB
@Thickness 0.0579 in
UL File Number E92442
 
Processing PropertiesMetricEnglishComments
Processing Temperature 260 - 282 °C500 - 540 °F
Rear Barrel Temperature 255 - 270 °C491 - 518 °F
Middle Barrel Temperature 260 - 277 °C500 - 531 °F
Front Barrel Temperature 266 - 282 °C511 - 540 °F
Nozzle Temperature 257 - 265 °C495 - 509 °F
Mold Temperature 38.0 - 82.0 °C100 - 180 °F
Drying Temperature 116 - 127 °C241 - 261 °F
Dry Time 6 - 8 hour6 - 8 hour
Moisture Content <= 0.015 %<= 0.015 %
Dew Point <= -17.8 °C<= 0.000 °F
Drying Air Flow Rate 22.7 - 28.3 l/min0.800 - 1.00 ft³/min (CFM)per lb/hour resin processed
Injection Pressure 68.9 - 138 MPa10000 - 20000 psi
Back Pressure 0.000 - 0.517 MPa0.000 - 75.0 psi
Cushion 0.635 cm0.250 in
Screw Speed 20 - 50 rpm20 - 50 rpm
 
Descriptive Properties
Fill RateModerate - Fast
Hold Pressure40 - 60% of injection pressure
Packing Pressure50 - 75% of injection pressure

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lotte Advanced Materials Infino® AE-2230 PC/PET, 20% MF
Covestro Makroblend® AR205 PC+PET
Lotte Advanced Materials Infino® AE-2150 PC/PET, 15% MF
Cheng Yu Plastic E500 PC/PET
Cheng Yu Plastic E500G10 PC/PET, 10% Glass Fiber

PMRC953 / 21007

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.