MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Armstrong A-706 Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, Cast, Metal Filled

Material Notes: A one-component, gray, aluminum-filled, thixotropic, non-sag epoxy adhesive. A-706 has an in-service temperature range to 400°F, but requires 350°F minimum cure temperature. Features excellent machining and tensile properties at room temperature. A-706 is qualified under Mil. Spec. MMM-A-134, Type III.

Information provided by Ellsworth Adhesives.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 160000 cP160000 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8686
Tensile Strength, Ultimate 59.6 MPa8650 psiafter optimum cure
Elongation at Break 2.4 %2.4 %
Adhesive Bond Strength 34.1 MPa4950 psiSteel-Steel; after optimum cure
 19.3 MPa
@Temperature -54.4 °C
2800 psi
@Temperature -66.0 °F
Aluminum-Aluminum tensile shear
 27.9 MPa
@Temperature 82.2 °C
4050 psi
@Temperature 180 °F
Aluminum-Aluminum tensile shear
 42.1 MPa
@Temperature 25.0 °C
6100 psi
@Temperature 77.0 °F
Aluminum-Aluminum tensile shear
 
Thermal PropertiesMetricEnglishComments
CTE, linear 53.0 µm/m-°C
@Temperature 20.0 °C
29.4 µin/in-°F
@Temperature 68.0 °F
Maximum Service Temperature, Air 204 °C400 °FAfter 350°F minimum cure temp.
Glass Transition Temp, Tg 130 °C266 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 177 °C350 °FOptimum cure is 2 hr. @ 350°F
 260 °C500 °FFast cure is 10 min. @ 500°F
Pot Life 99999 min
@Temperature 25.0 °C
99999 min
@Temperature 77.0 °F
Indefinite working life at 25°C (100 g)
 
Descriptive Properties
ColorAmber
Mix Ratio1 Part

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AorTech Biomaterials Elast-Eon™ E2A Biomedical Polyurethane Pellets
AorTech Biomaterials Elast-Eon™ E2-945 Biomedical Polyurethane Pellets
AorTech Biomaterials Elast-Eon™ E2-852 Biomedical Polyurethane Pellets
Atom Adhesives AA-BOND 428 Epoxy Adhesive
Armstrong A-701 Epoxy Adhesive

PARM26 / 24558

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.