MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Jushi UD1200 Glass Fiber Epoxy Composite
Categories: Polymer; Thermoset; Epoxy; Epoxy, Molded, Glass Fiber Filler

Material Notes: UD1200 is made using Jushi E7 glass. Compared to traditional E Glass, E7 has 30% higher strength, 23% higher modulus, and a higher softening point. It offers better corrosion resistance than B-free E glass in acid, alkaline, and neutral aqueous solutions.

Data for laminate with UD1200 fabric using epoxy vacuum infusion process.

Information provided by Jushi Group Co. Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Filler Content 54 %54 %UD1200
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 1229 MPa178300 psi0°; ISO 527-5
Tensile Modulus 41.3 GPa5990 ksi0°; ISO 527-5
Compressive Strength 850 MPa123000 psi0°; ISO 14126
Compressive Modulus 46.6 GPa6760 ksi0°; ISO 14126
Fatigue Strength  375 MPa
@# of Cycles 1.00e+7
54400 psi
@# of Cycles 1.00e+7
 500 MPa
@# of Cycles 500000
72500 psi
@# of Cycles 500000
 625 MPa
@# of Cycles 50000
90600 psi
@# of Cycles 50000
 750 MPa
@# of Cycles 5000
109000 psi
@# of Cycles 5000
Shear Modulus 4.10 GPa595 ksi45°; ISO 14129
Shear Strength 51.0 MPa7400 psi45°; ISO 14129

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Quantum Composites Lytex® 9063 63% Glass Fiber Epoxy SMC
Jushi E7 DR-380 Direct Roving - Epoxy Composite
Jushi E7 DR-386T Direct Roving - Epoxy Composite
Owens Corning Glass Fiber Reinforced Epoxy (Filament Wound), 80 wt.% glass
DuPont Mobility and Materials Vespel® CP-9800 Carbon Fiber and Epoxy Composite, Ultra-high modulus end effectors

PJUSHI990 / 183361

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.