MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis Daplen™ EE065AI Polypropylene Elastomer Modified  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Mineral Reinforced

Material Notes: Daplen™ EE065AI is an elastomer modified polypropylene with increased crystallinity. This material has an excellent balance between impact strength and stiffness. The product is available in natural color. Applications: automotive interior parts including door panels and pockets, and center consoles.

Information provided by Borealis AG

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.905 g/cc0.0327 lb/in³ISO 1183
Linear Mold Shrinkage 0.015 cm/cm0.015 in/inBorealis Method
Melt Flow 11.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
11.5 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 43.0 MPa6240 psiH 358/30; ISO 2039
Tensile Strength at Break 15.0 MPa2180 psiISO 527-2
Tensile Strength, Yield 21.0 MPa3050 psi50mm/min; ISO 527-2
Elongation at Break 150 %150 %50mm/min; ISO 527-2
Elongation at Yield 5.1 %5.1 %50mm/min; ISO 527-2
Tensile Modulus 1.10 GPa160 ksi1mm/min; ISO 527-2
Flexural Strength 22.5 MPa3260 psi3.5% strain; ISO 178
 25.0 MPa3630 psiISO 178
Flexural Modulus 1.00 GPa145 ksi2mm/min; ISO 178
Izod Impact, Notched (ISO)  8.50 kJ/m²
@Temperature -20.0 °C
4.04 ft-lb/in²
@Temperature -4.00 °F
ISO 180/1A
 50.0 kJ/m²
@Temperature 23.0 °C
23.8 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Izod Impact, Unnotched (ISO)  200 kJ/m²
@Temperature -20.0 °C
95.2 ft-lb/in²
@Temperature -4.00 °F
ISO 180/1U
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 180/1U
Charpy Impact Unnotched  22.0 J/cm²
@Temperature -20.0 °C
105 ft-lb/in²
@Temperature -4.00 °F
ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.900 J/cm²
@Temperature -20.0 °C
4.28 ft-lb/in²
@Temperature -4.00 °F
ISO 179/1eA
 5.50 J/cm²
@Temperature 23.0 °C
26.2 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 82.0 °C180 °FISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 53.0 °C127 °FISO 75-2
Vicat Softening Point  56.0 °C
@Load 5.10 kg
133 °F
@Load 11.2 lb
ISO 306
 143 °C
@Load 1.02 kg
289 °F
@Load 2.25 lb
ISO 306
 
Processing PropertiesMetricEnglishComments
Feed Temperature 40.0 - 80.0 °C104 - 176 °F
Melt Temperature 220 - 260 °C428 - 500 °Fmass temperature
Mold Temperature 30.0 - 50.0 °C86.0 - 122 °F
Injection Velocity 100 - 200 mm/sec3.94 - 7.87 in/sec
Hold Pressure 3.00 - 6.00 MPa435 - 870 psi
 
Descriptive Properties
Back Pressurelow to medium
Emission (µgC/g)< 50VDA 227
Fogging (mg)<2DIN 75201
Screw Speedlow to medium

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Exxtral™ CNU 011 Performance Polyolefin
LyondellBasell Hifax TKS 2050P S81536 Polypropylene Elastomer
Borealis Daplen™ EE002AE Polypropylene Elastomer Modified
LyondellBasell Hostacom EKG 286T BLACK Polypropylene , Elastomer Modified
Overview of materials for High Density Polyethylene (HDPE), Film Grade

PBOREA406 / 108665

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.