MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Epoxy Technology EPO-TEK® T7139 Glob Top Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Product Description: EPO-TEK® T7139 is a two component, electrically insulating, encapsulating epoxy designed for semiconductor glob top applications and package assembly.

Advantages & Application Notes:

  • A pot life of at least one day is mass production friendly and convenient for consecutive manufacturing shifts.
  • Its thixotropic nature allows for dispensing “domes or hemispheres” directly over the IC without the need for using a dam or cavity to control flow.
  • Suggested Applications:
    • Semiconductor:
      • Glob top encapsulant for COB die attach.
      • Plastic semiconductor package filling instead of traditional epoxy transfer molding compound.
    • Electronic/PCB: general protection of SMDs.
    • Opto-electronics: black and opaque epoxy for adhesive and sealing applications while blocking IR and VIS light.
  • In some cases, it is advantageous to pre-warm the epoxy < 50°C in order to decrease its thixotropic nature, while increasing capillary and flow rate.
  • Low CTE makes it ideal for keeping stresses to a minimum.

Information Provided by Epoxy Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.31 g/cc1.31 g/ccPart A
 1.34 g/cc1.34 g/ccPart B
Particle Size <= 50 µm<= 50 µm
Viscosity 5000 - 7000 cP
@Temperature 23.0 °C
5000 - 7000 cP
@Temperature 73.4 °F
50 rpm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8686
Tensile Modulus 4.13 GPa599 ksiStorage
Shear Strength 13.8 MPa2000 psiLap
 >= 23.4 MPa>= 3400 psiDie
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 3.00e+12 ohm-cm>= 3.00e+12 ohm-cm
Dielectric Constant 3.39
@Frequency 1000 Hz
3.39
@Frequency 1000 Hz
Dissipation Factor 0.0060
@Frequency 1000 Hz
0.0060
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 30.0 µm/m-°C16.7 µin/in-°FBelow Tg
 76.0 µm/m-°C42.2 µin/in-°FAbove Tg
Thermal Conductivity 0.430 W/m-K2.98 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 250 °C482 °FContinuous
 350 °C662 °FIntermittent
Minimum Service Temperature, Air -55.0 °C-67.0 °FContinuous
 -55.0 °C-67.0 °FIntermittent
Glass Transition Temp, Tg >= 90.0 °C>= 194 °FDynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min
Decomposition Temperature 438 °C820 °FDegradation Temperature
 
Optical PropertiesMetricEnglishComments
Transmission, Visible  <= 0.010 %
@Wavelength 400 nm
<= 0.010 %
@Wavelength 400 nm
 <= 1.0 %
@Wavelength 900 nm
<= 1.0 %
@Wavelength 900 nm
 <= 5.0 %
@Wavelength 2000 nm
<= 5.0 %
@Wavelength 2000 nm
 
Processing PropertiesMetricEnglishComments
Cure Time  30.0 min
@Temperature 150 °C
0.500 hour
@Temperature 302 °F
Minimum Bond Line
 60.0 min
@Temperature 125 °C
1.00 hour
@Temperature 257 °F
Minimum Bond Line
Pot Life 1440 min1440 min
Shelf Life 12.0 Month
@Temperature 25.0 °C
12.0 Month
@Temperature 77.0 °F
 
Descriptive Properties
ColorBlackPart A
 TanPart B
ConsistencySmooth paste
Mix Ratio by Weight10:1
Number of ComponentsTwo
Thixotropic Index2.5
Weight Loss0.19%200°C
 0.34%250°C
 0.48%300°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® H67-MP Thermally Conductive Epoxy
Epoxy Technology EPO-TEK® H67MP-GB Thermally Conductive, Electrically Insulating Epoxy
Henkel Loctite® 3534 Glob Top Encapsulant
Vyncolit Neopreg Kinel® SK80 L8G Glass Fiber Reinforced Molding Compound
Epoxy Technology EPO-TEK® H55 Epoxy

PPOXYT097 / 141136

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.