MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Epoxy Technology EPO-TEK® H67MP-GB Thermally Conductive, Electrically Insulating Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy, Thermally Conductive

Material Notes: Preliminary Product Information Sheet

Material Description: A single component, thermally conductive, electrically insulating epoxy designed to meet the requirements of MIL-STD-883/Test Method 5011 for hybrid microelectronic packaging and assemblies. It maybe used for bonding SMDs, die-attach, substrate-attach or general heat sinking. It is a version of EPO-TEK® H67MP which contains 2 mil glass beads.

Information Provided by Epoxy Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.00 g/cc2.00 g/cc
Particle Size <= 55 µm<= 55 µm
Viscosity 334200 cP
@Temperature 23.0 °C
334200 cP
@Temperature 73.4 °F
1 rpm
 
Chemical PropertiesMetricEnglishComments
Ionic Impurities - Na (Sodium) <= 50 ppm<= 50 ppm
Ionic Impurities - K (Potassium) <= 50 ppm<= 50 ppm
Ionic Impurities - Cl (Chloride) <= 200 ppm<= 200 ppm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8686
Tensile Modulus 5.8765 GPa852.31 ksiStorage
Shear Strength >= 13.8 MPa>= 2000 psiLap
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 2.00e+13 ohm-cm>= 2.00e+13 ohm-cm
Dielectric Constant 5.01
@Frequency 1000 Hz
5.01
@Frequency 1000 Hz
Dissipation Factor 0.0045
@Frequency 1000 Hz
0.0045
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.0 µm/m-°C9.44 µin/in-°FBelow Tg
 75.0 µm/m-°C41.7 µin/in-°FAbove Tg
Thermal Conductivity 0.430 W/m-K2.98 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 200 °C392 °FContinuous
 300 °C572 °FIntermittent
Minimum Service Temperature, Air -55.0 °C-67.0 °FContinuous
 -55.0 °C-67.0 °FIntermittent
Glass Transition Temp, Tg >= 93.0 °C>= 199 °F
Decomposition Temperature 360 °C680 °FDegradation Temperature
 
Processing PropertiesMetricEnglishComments
Cure Time 60.0 min
@Temperature 150 °C
1.00 hour
@Temperature 302 °F
Minimum Bond Line
Pot Life 40320 min40320 min
Shelf Life 12.0 Month
@Temperature -40.0 °C
12.0 Month
@Temperature -40.0 °F
 
Descriptive Properties
ColorWhite
ConsistencyHighly viscous paste
Ionic Impurities NH444 ppm
Number of ComponentsSingle
Weight Loss0.29%200°C
 0.79%250°C
 1.62%300°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® H61LV Thermally Conductive, Electrically Insulating Epoxy
Epoxy Technology EPO-TEK® H63 Thermally Conductive, Electrically Insulating Epoxy
Epoxy Technology EPO-TEK® H61ND Thermally Conductive, Electrically Insulating Epoxy
Epoxy Technology EPO-TEK® B9021-13 Thermally Conductive, Electrically Insulating Epoxy
Epoxy Technology EPO-TEK® H73 Thermally Conductive, Electrically Insulating Epoxy

PPOXYT069 / 141108

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.