MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexPly® 916 120°C Curing Epoxy Matrix
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: HexPly® 916 is a self-extinguishing modified epoxy matrix system with very high self adhesive properties. It is an ideal system for single shot honeycomb sandwich manufacture, with good drape characteristics. HexPly® 916 exhibits excellent environmental resistance, and good service temperature capability.
HexPly® 916 prepregs are only available in fabric form.

Features: Self-extinguishing, High strength retention to 120°C, Excellent adhesion to honeycomb, Suitable for a range of cure pressure (0.8 to 10 bar), Tough matrix system, Low tack

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³Cured
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 50.0 MPa7250 psiISO R527 type 1
Elongation at Yield 1.4 %1.4 %ISO R527 type 1
Tensile Modulus 4.17 GPa605 ksiISO R527 type 1
Flexural Yield Strength 92.0 MPa13300 psiISO 178
Flexural Modulus 3.78 GPa548 ksiISO 178
Compressive Strain at Yield 10.3 %10.3 %ISO 604
Compressive Yield Strength 151.7 MPa22000 psiISO 604
Shear Modulus 1.52 GPa220 ksiISO R527 type 1
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 145 °C293 °FDMTA
 
Processing PropertiesMetricEnglishComments
Shelf Life >= 12.0 Month
@Temperature -18.0 °C
>= 12.0 Month
@Temperature -0.400 °F
 
Descriptive Properties
Tack Life (days)30

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexPly® 171/174/176 120°C Curing Epoxy Matrix
Hexcel® HexPly® 6376 175°C Curing Epoxy Matrix
Hexcel® HexPly® 920 125°C Curing Epoxy Matrix
Hexcel® HexPly® 914 175°C Curing Epoxy Matrix
Hexcel® HexPly® 913 125°C Curing Epoxy Matrix

PHEXC060 / 98530

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.