MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Dow Tyril® 125 SAN  (discontinued **)
Categories: Polymer; Thermoplastic; SAN Polymer; Styrene Acrylonitrile (SAN), Molded

Material Notes: Dow TYRIL® 125 resin is specially formulated for blending and is an ideal carrier material for use in making color concentrates. It offers high melt flow and excellent chemical resistance.

Data provided by Dow Chemical.

Tyril is now a Trinseo product line; this specific grade was discontinued while still a Dow product.

Key Words: Poly(Styrene Acrylonitrile)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³ASTM Data
Melt Density 0.914 g/cc0.0330 lb/in³
Melt Flow 25 g/10 min
@Load 3.80 kg,
Temperature 230 °C
25 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM Data
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 45.0 MPa6530 psiASTM Data
Tensile Strength, Yield 45.0 MPa6530 psiASTM Data
Elongation at Break 1.5 %1.5 %ASTM Data
Tensile Modulus 3.31 GPa480 ksiASTM Data
Charpy Impact Unnotched 1.00 J/cm²4.76 ft-lb/in²ISO Data
 1.00 J/cm²4.76 ft-lb/in²ISO Data, Low Temp
Charpy Impact, Notched 0.100 J/cm²0.476 ft-lb/in²ISO Data, Low Temp
 0.200 J/cm²0.952 ft-lb/in²ISO Data
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 63.0 µm/m-°C
@Temperature 20.0 °C
35.0 µin/in-°F
@Temperature 68.0 °F
ISO data
Specific Heat Capacity 1.68 J/g-°C0.402 BTU/lb-°F
Thermal Conductivity 0.113 W/m-K0.784 BTU-in/hr-ft²-°F
Deflection Temperature at 0.46 MPa (66 psi) 99.0 °C210 °FUnannealed; ASTM Data
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C185 °FUnannealed; ASTM Data
Vicat Softening Point 113 °C235 °F
 
Optical PropertiesMetricEnglishComments
Haze 0.45 %0.45 %
Transmission, Visible 91 %91 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution Luran® HD-20 SAN
Dow Tyril® 100 SAN
INEOS Styrolution Terlux® HD 2822 Methyl Methacrylate Acrylonitrile Butadiene Styrene (MABS)
Chi Mei Kibisan® PN-117C SAN
Dow Tyril® 880 SAN

PDW183 / 34414

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.