MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

INEOS Styrolution Terlux® HD 2822 Methyl Methacrylate Acrylonitrile Butadiene Styrene (MABS)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Terlux® HD 2822 is a new standard-injection molding grade based on a MABS polymer. Terlux® HD 2822 offers a well balanced combination of stiffness and toughness and the high transparency well known in SAN molding compositions. Excellent transparency, Good resistance to chemicals, Good Stiffness and surface finish, High impact strength, HD service package available. Applications: Medical devices

Information provided by Styrolution.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.590 g/cc0.0213 lb/in³with external lubricant
Density 1.08 g/cc0.0390 lb/in³ISO 1183
Water Absorption at Saturation 0.70 %
@Temperature 23.0 °C
0.70 %
@Temperature 73.4 °F
ISO 62
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inISO 294-4
Melt Flow  2.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
2.0 g/10 min
@Load 22.0 lb,
Temperature 428 °F
Volumetric; cm3/10 min; ISO 1133
 17 g/10 min
@Load 21.6 kg,
Temperature 220 °C
17 g/10 min
@Load 47.6 lb,
Temperature 428 °F
Volumetric; cm3/10 min; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 70.0 MPa10200 psiISO 2039-1
Tensile Strength, Yield 48.0 MPa6960 psiISO 527
Elongation at Break 12 %12 %Nominal; ISO 527
Elongation at Yield 4.0 %4.0 %ISO 527
Tensile Modulus 2.00 GPa290 ksiISO 527
Flexural Strength 70.0 MPa10200 psiISO 178
Charpy Impact Unnotched  8.00 J/cm²
@Temperature -30.0 °C
38.1 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 12.0 J/cm²
@Temperature 23.0 °C
57.1 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.200 J/cm²
@Temperature -30.0 °C
0.952 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.500 J/cm²
@Temperature 23.0 °C
2.38 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Tensile Creep Modulus, 1000 hours 1250 MPa181000 psiISO 899
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohm1.00e+15 ohmIEC 60093
Dielectric Constant 2.9
@Frequency 100 Hz
2.9
@Frequency 100 Hz
IEC 60250
Dissipation Factor  0.014
@Frequency 1e+6 Hz
0.014
@Frequency 1e+6 Hz
IEC 60250
 0.016
@Frequency 100 Hz
0.016
@Frequency 100 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 - 110 µm/m-°C44.4 - 61.1 µin/in-°FISO 11359
Thermal Conductivity 0.170 W/m-K1.18 BTU-in/hr-ft²-°FDIN 52612-1
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C201 °Fannealed 4 hours at 80°C; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C194 °Fannealed 4 hours at 80°C; ISO 75
Vicat Softening Point  93.0 °C
@Load 5.10 kg
199 °F
@Load 11.2 lb
VST/B/50. 50C/h; ISO 306
 105 °C
@Load 1.02 kg
221 °F
@Load 2.25 lb
VST/A/50. 50C/h; ISO 306
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.541.54Sodium D Line; ISO 489
 
Processing PropertiesMetricEnglishComments
Melt Temperature 230 - 260 °C446 - 500 °FISO 294
Mold Temperature 50.0 - 75.0 °C122 - 167 °FISO 294
Injection Velocity 200 mm/sec7.87 in/secISO 294
Drying Temperature 70.0 °C
@Time 7200 sec
158 °F
@Time 2.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Tyril® 100 SAN
INEOS Styrolution Luran® HD-20 SAN
INEOS Styrolution K-Resin® KR01 Styrene Butadiene Copolymer (SBC)
Dow Tyril® 125 SAN
INEOS Styrolution Terlux® HD 2802 MABS

PSTYR9864 / 216091

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.