MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik SITREN® PSR 100 Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product description: SITREN® PSR 100 is a powdered shrinkage reducing additive. The active components are organic alcohols on an inorganic carrier.

Applications: SITREN® P 750 may be used in a variety of cementitious drymix applications where the application of conventional liquid water repellents is not feasible or desired, e. g.:

  • Tile grouts
  • Plasters
  • Renders
  • Sealing slurries SITREN® PSR 100 reduces the drying shrinkage and the autogenous shrinkage of cementitious, dry-mix and specialty mortar formulations, that can occur when the formulation is losing moisture during the drying process.

    Properties/Benefits: In cementitious and concrete formulations SITREN® PSR 100 reduces the surface tension of pore fluids. As a result it provides the following benefits,

    • SITREN® PSR 100 reduces significantly the drying shrinkage and the autogenous shrinkage
    • SITREN® PSR 100 reduces the magnitude of capillary stresses and shrinkage strains
    • SITREN® PSR 100 improves the crack resistance
    • SITREN® PSR 100 can significantly improve the resistance to chloride ion diffusivity
    • SITREN® PSR 100 has no negative effect on the workability

    Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.550 g/cc0.0199 lb/in³
 
Descriptive Properties
Appearancewhite, free flowing powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium Aluminum Nitride (TiAlN) PVD Coating
Evonik TEGOPREN® 5878 Additive
Evonik SITREN® P 750 Water repellent
Evonik SITREN® AirVoid® 354 Surfactant
Evonik Protectosil® Degadeck® CSS Surface Treatment

PEVONIM179 / 197383

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.