MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik Protectosil® Degadeck® CSS Surface Treatment
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: Product Description: Protectosil Degadeck CSS is a low viscosity reactive methymethacrylate (MMA) for use in sealing cracks in concrete structures. Protectosil Degadeck CSS is a two component liquid material which is catalyzed to cure into a hard methylmethacrylate (MMA) resin. The low viscosity of the Protectosil Degadeck CSS allows it to readily penetrate into cracks. Cracks as wide as 1/8 of an inch (3 mm) to hairline can be sealed. Protectosil Degadeck CSS cures within one hour and is ready for traffic at that time. The cured MMA is resistant to wear, chloride ion ingress, and also alkali attack. Protectosil Degadeck CSS penetrates into cracks, then reacts to seal against water an chloride ion intrusion. The unique MMA resin also seals sound concrete against water and chloride ion ingress. The cured MMA creates a barrier which prevents the ingress of water and waterborne contaminants from entering the substrate and causing premature deterioration. By combining the two low viscosity components of the MMA resin, Protectosil Degadeck CSS penetrates by gravity into even the smallest crack. The excellent adhesion and strength of the cured resin ensures a long service life.

Applications: For use to seal cracks on cast-in-place, pre-cast, and high strength concrete as well as concrete surfaces from ingress of water and waterborne contaminates, such as chloride ions. For use on concrete bridge decks, parking garages, pedestrian walkways and other elevated concrete.

Advantages: Protectosil Degadeck CSS is a 100% solid reactive MMA resin with low intrinsic viscosity and excellent adhesion to concrete surfaces. The main benefits of the product are:

  • Fast Curing System
  • Deep penetration into cracks
  • Excellent adhesion and bond strength
  • Excellent water and chloride ion screening
  • Compatible with other Protectosil Building Protection products
  • UV Resistance
  • Highly resistant to alkali attack

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatile Organic Compounds (VOC) Content <= 70 g/l<= 70 g/l
Viscosity 5.0 - 15 cP5.0 - 15 cP
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 54.0 MPa7830 psiDIN EN ISO 527
Elongation at Break 4.0 %4.0 %DIN EN ISO 527
Flexural Strength 2.00 MPa290 psiDIN EN ISO 1788
 
Thermal PropertiesMetricEnglishComments
Flash Point 10.0 °C50.0 °F
 
Processing PropertiesMetricEnglishComments
Pot Life  5.00 - 10.0 min
@Temperature 32.0 °C
5.00 - 10.0 min
@Temperature 89.6 °F
 12.0 - 16.0 min
@Temperature 9.00 °C
12.0 - 16.0 min
@Temperature 48.2 °F
 15.0 min
@Temperature 9.00 °C
15.0 min
@Temperature 48.2 °F
 15.0 - 20.0 min
@Temperature 16.0 °C
15.0 - 20.0 min
@Temperature 60.8 °F
 15.0 - 20.0 min
@Temperature 21.0 °C
15.0 - 20.0 min
@Temperature 69.8 °F
 20.0 - 25.0 min
@Temperature 27.0 °C
20.0 - 25.0 min
@Temperature 80.6 °F
 
Descriptive Properties
Colorbluish, slightly turbid liquid
Content100%active

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium Aluminum Nitride (TiAlN) PVD Coating
Evonik TEGOPREN® 5878 Additive
Evonik SITREN® PSR 100 Additive
Evonik SITREN® P 750 Water repellent
Evonik SITREN® AirVoid® 354 Surfactant

PEVONIM133 / 197337

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.