MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Telcar® TL-3954-62 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Vinyl (PVC); PVC, Wire and Cable Grade

Material Notes: Notes: Telcar TL-3954-62 is a general purpose thermoplastic elastomer designed for a variety of wire and cable applications, including cable jacketing and cable insulation. Telcar TL-3954-62 is a medium hardness, high density grade that is RoHS compliant grade that is suitable for both injection molding and extrusion.

Features: Filled; General Purpose; Good Mold Release: Good Moldability; Good Processability; High Density; High Specific Gravity; Low Flow; Medium Hardness

Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Construction Applications; Flexible Cord Jacketing; Industrial Applications; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire and Cable Applications; Wire Jacketing

Forms: Pellets

Processing Method: Extrusion; Injection Molding

Injection Notes: Injection Rate: Moderate-Fast

Extrusion Notes: Screw Speed: 30 to 100 rpm

Information Provided by Teknor Apex

Key Words: TPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.18 g/cc1.18 g/ccASTM D792
Melt Flow 1.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
1.5 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  60
@Time 5.00 sec
60
@Time 0.00139 hour
Injection Molded; ASTM D2240
 62
@Time 1.00 sec
62
@Time 0.000278 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 6.15 MPa892 psiFlow, Die C, 20 in/min; ASTM D412
 7.79 MPa1130 psiAcross Flow, Die C, 20 in/min; ASTM D412
Tensile Stress at Strain  1.54 MPa
@Strain 100 %
223 psi
@Strain 100 %
Across Flow, Die C, 20 in/min; ASTM D412
 2.08 MPa
@Strain 100 %
301 psi
@Strain 100 %
Flow, Die C, 20 in/min; ASTM D412
 2.42 MPa
@Strain 300 %
351 psi
@Strain 300 %
Across Flow, Die C, 20 in/min; ASTM D412
 2.99 MPa
@Strain 300 %
433 psi
@Strain 300 %
Flow, Die C, 20 in/min; ASTM D412
Elongation at Break 670 %670 %Flow, Die C, 20 in/min; ASTM D412
 730 %730 %Across Flow, Die C, 20 in/min; ASTM D412
Tear Strength 26.1 kN/m149 pliFlow, Die C, 20 in/min; ASTM D624
 27.5 kN/m157 pliAcross Flow, Die C, 20 in/min; ASTM D624
Compression Set  26 %
@Temperature 22.8 °C,
Time 79200 sec
26 %
@Temperature 73.0 °F,
Time 22.0 hour
Type 1; ASTM D395B
 46 %
@Temperature 70.0 °C,
Time 79200 sec
46 %
@Temperature 158 °F,
Time 22.0 hour
Type 1; ASTM D395B
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -60.0 °C<= -76.0 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 171 - 193 °C340 - 380 °F
Middle Barrel Temperature 177 - 199 °C350 - 390 °F
Front Barrel Temperature 182 - 204 °C360 - 400 °F
Nozzle Temperature 188 - 210 °C370 - 410 °F
Zone 1 166 - 188 °C330 - 370 °F
Zone 2 171 - 193 °C340 - 380 °F
Zone 3 177 - 199 °C350 - 390 °F
Zone 4 350 - 390 °C662 - 734 °F
Zone 5 182 - 204 °C360 - 400 °F
Die Temperature 190 - 210 °C374 - 410 °F
Melt Temperature 188 - 210 °C370 - 410 °FProcessing Temperature
Mold Temperature 25.0 - 65.6 °C77.0 - 150 °F
Injection Pressure 1.38 - 6.89 MPa200 - 1000 psi
Back Pressure 0.172 - 0.345 MPa25.0 - 50.0 psi
Cushion 0.381 - 2.54 cm0.150 - 1.00 in
Screw Speed 50 - 100 rpm50 - 100 rpm
 
Descriptive Properties
AppearanceOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Sarlink® 4380 Thermoplastic Elastomer
Overview of materials for PVC, Flexible Grade
Avient ProFlex™ MB NP70/30 Nitrile/PVC Elastomer (NBR/PVC) Compound
Armacell Ensolite™ AG2 Continuous Rolls/Sheets, PVC/NBR
AlphaGary Garaflex™ E X 00-207F UV-FG LCF Vinyl Thermoplastic Elastomer

PTEKNP500 / 129581

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.