MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow DOWLEX™ 2267G Linear Low Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes:
  • A high performance stretch film resin
  • Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.917 g/cc0.0331 lb/in³ASTM D792
Thickness 20.3 microns0.800 mil
Melt Flow 0.85 g/10 min0.85 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 9.218 MPa1337 psiASTM D882
Film Tensile Strength at Yield, TD 9.501 MPa1378 psiASTM D882
Film Elongation at Break, MD 421 %421 %ASTM D882
Film Elongation at Break, TD 608 %608 %ASTM D882
Secant Modulus, MD 0.1494 GPa21.67 ksi2% Secant; ASTM D882
Secant Modulus, TD 0.15536 GPa22.533 ksi2% Secant; ASTM D882
Impact 130130[ft-lbf/in3]; Puncture Resistance; Dow Method
 765765[ft-lbf/in3]; Toughness MD; ASTM D882
 918918[ft-lbf/in3]; Toughness TD; ASTM D882
Elmendorf Tear Strength MD 323 g323 gASTM D1922
Elmendorf Tear Strength TD 518 g518 gASTM D1922
Elmendorf Tear Strength, MD 15.896 g/micron403.75 g/milASTM D1922
Elmendorf Tear Strength, TD 25.49 g/micron647.5 g/milASTM D1922
Dart Drop Test 474 g1.05 lbMethod A; ASTM D1709
Film Tensile Strength at Break, MD 33.34 MPa4835 psiASTM D882
Film Tensile Strength at Break, TD 25.66 MPa3722 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 122 °C252 °FDow Method (DSC)
Vicat Softening Point 102 °C216 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 9.0 %9.0 %ASTM D1003
Gloss 65 %65 %45°; ASTM D2457
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow DOWLEX™ 2045G Linear Low Density Polyethylene
Dow DOWLEX™ 2020G Linear Low Density Polyethylene
Dow DOWLEX™ 2021D Linear Low Density Polyethylene
Dow DOWLEX™ 2038 Linear Low Density Polyethylene
Dow DOWLEX™ 2070G Linear Low Density Polyethylene

PDOW1319 / 30537

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.