MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aluminum 2014-O
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 2000 Series Aluminum Alloy

Material Notes: Used in applications requiring high strength/hardness, including elevated temperature uses. Specific applications include heavy duty forgings, plate, and extrusions for aerospace fittings, wheels, tanks, and major structural components, heavy duty automotive frame and suspension componentry. 2014 exhibits poor corrosion resistance for an aluminum alloy.

Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
A Zr + Ti limit of 0.20 percent maximum may be used with this alloy designation for extruded and forged products only, but only when the supplier and the purchaser have mutually agreed.
Composition information provided by the Aluminum Association and is not for design.

Key Words: Aluminium 2014-O; UNS A92014; ISO AlCu4SiMg; BS H15 (UK); CSA CS41N (Canada); AA2014-O, DIN AlCuSiMn; NF A-U4SG (France); Al2014-O
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.80 g/cc0.101 lb/in³AA; Typical
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 4545AA; Typical; 500 g load; 10 mm ball
Tensile Strength, Ultimate 186 MPa27000 psiAA; Typical
 <= 205 MPa<= 29700 psiExtruded wire, rod, bar, and shapes
 <= 205 MPa<= 29700 psiExtruded tube
 <= 220 MPa
@Thickness 0.508 - 12.7 mm
<= 31900 psi
@Thickness 0.0200 - 0.499 in
Sheet and plate
 <= 220 MPa
@Thickness 12.7 - 25.4 mm
<= 31900 psi
@Thickness 0.500 - 1.00 in
Sheet and plate
 <= 220 MPa
@Thickness 4.57 - 12.7 mm
<= 31900 psi
@Thickness 0.180 - 0.500 in
Drawn tube
Tensile Strength, Yield 96.5 MPa14000 psiAA; Typical
 <= 125 MPa<= 18100 psiExtruded wire, rod, bar, and shapes
 <= 125 MPa<= 18100 psiExtruded tube
 <= 110 MPa
@Thickness 0.508 - 12.7 mm
<= 16000 psi
@Thickness 0.0200 - 0.499 in
Sheet and plate
 <= 110 MPa
@Thickness 4.57 - 12.7 mm
<= 16000 psi
@Thickness 0.180 - 0.500 in
Drawn tube
Elongation at Break 12 %12 %Extruded wire, rod, bar, and shapes
 12 %12 %Extruded tube
 10 %
@Thickness 12.7 - 25.4 mm
10 %
@Thickness 0.500 - 1.00 in
Sheet and plate
 16 %
@Thickness 0.508 - 12.7 mm
16 %
@Thickness 0.0200 - 0.499 in
Sheet and plate
 18 %
@Diameter 12.7 mm
18 %
@Diameter 0.500 in
AA; Typical
Modulus of Elasticity 73.1 GPa10600 ksiAA; Typical; Average of tension and compression. Compression modulus is about 2% greater than tensile modulus.
Tensile Modulus 72.4 GPa10500 ksi
Compressive Strength 185 MPa26800 psi
Compressive Modulus 73.8 GPa10700 ksi
Poissons Ratio 0.330.33
Fatigue Strength 89.6 MPa
@# of Cycles 5.00e+8
13000 psi
@# of Cycles 5.00e+8
completely reversed stress; RR Moore machine/specimen
Machinability 30 %30 %0-100 Scale of Aluminum Alloys
Shear Modulus 28.0 GPa4060 ksi
Shear Strength 124 MPa18000 psiAA; Typical
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000349 ohm-cm
@Temperature 20.0 °C
0.00000349 ohm-cm
@Temperature 68.0 °F
AA; Typical
 
Thermal PropertiesMetricEnglishComments
CTE, linear  20.8 µm/m-°C
@Temperature -50.0 - 20.0 °C
11.6 µin/in-°F
@Temperature -58.0 - 68.0 °F
 22.5 µm/m-°C
@Temperature 20.0 - 100 °C
12.5 µin/in-°F
@Temperature 68.0 - 212 °F
 23.0 µm/m-°C
@Temperature 20.0 - 100 °C
12.8 µin/in-°F
@Temperature 68.0 - 212 °F
AA; Typical; average over range
 23.4 µm/m-°C
@Temperature 20.0 - 200 °C
13.0 µin/in-°F
@Temperature 68.0 - 392 °F
 24.4 µm/m-°C
@Temperature 20.0 - 300 °C
13.6 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.880 J/g-°C0.210 BTU/lb-°FEstimated from trends in similar Al alloys.
Thermal Conductivity 193 W/m-K1340 BTU-in/hr-ft²-°FAA; Typical at 77°F
Melting Point 507 - 638 °C945 - 1180 °FAA; Typical range based on typical composition for wrought products >= 1/4 in. thickness. Eutectic melting is not eliminated by homogenization.
Solidus 507 °C945 °FAA; Typical
Liquidus 638 °C1180 °FAA; Typical
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 413 °C775 °F
Solution Temperature 502 °C935 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 90.4 - 95 %90.4 - 95 %As remainder
Chromium, Cr <= 0.10 %<= 0.10 %
Copper, Cu 3.9 - 5.0 %3.9 - 5.0 %
Iron, Fe <= 0.70 %<= 0.70 %
Magnesium, Mg 0.20 - 0.80 %0.20 - 0.80 %
Manganese, Mn 0.40 - 1.2 %0.40 - 1.2 %
Other, each <= 0.05 %<= 0.05 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si 0.50 - 1.2 %0.50 - 1.2 %
Titanium, Ti <= 0.15 %<= 0.15 %
Zinc, Zn <= 0.25 %<= 0.25 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 2014-T4; 2014-T451
Aluminum 2014-T6; 2014-T651
Aluminum 2014-T3
DWA 6092/SiC/17.5p-T6 Aluminum SiC Metal-Matrix-Composite (Al MMC), Sheet
Aluminum 2014-T6; 2014-T651 (Extended Form Data)

MA2014O / 8845

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.