MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Goodfellow Reaction Bonded Silicon Nitride Si3N4
Categories: Ceramic; Nitride

Material Notes: Reaction Bonded Silicon Nitride is produced by nitriding compacted Silicon powder. This production route is considerably more cost-effective than hot-pressing. Very complex and accurate shapes can be produced, which hold their shape during firing. After firing, as for Hot Pressed Silicon Nitride, it can be diamond ground to tolerances as close as 0.01mm. Although not as strong as Hot Pressed Silicon Nitride, its strength is held up to 1400°C, with long term oxidation resistance up to 1150°C. The thermal and electrical properties of the two forms of Silicon Nitride are very similar. RBSN finds use as supports in situations of continuous temperature cycling within ranges of up to 1000°C, as well as for gas turbine components. Reaction Bonded Silicon Nitride is resistant to a wide range of chemicals and molten metals. Silicon Nitride spheres have found use as bearings in the automotive industry, as they have high wear resistance and have a coefficient of friction and a density much lower than steel.

Information provided by Goodfellow.

Key Words: Si3N4; RBSN, NITRASIL® R
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.40 g/cc0.0867 lb/in³
Porosity 15 - 23 %15 - 23 %Apparent
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 800 - 1000800 - 1000kgf/mm²
Tensile Modulus 170 - 220 GPa24700 - 31900 ksi
Compressive Strength 550 - 650 MPa79800 - 94300 psi
Shear Strength 190 - 240 MPa27600 - 34800 psi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+7 ohm-cm>= 1.00e+7 ohm-cm
Dielectric Constant 1010
 
Thermal PropertiesMetricEnglishComments
CTE, linear 3.30 µm/m-°C
@Temperature 20.0 - 1000 °C
1.83 µin/in-°F
@Temperature 68.0 - 1830 °F
Specific Heat Capacity 0.690 J/g-°C
@Temperature 25.0 °C
0.165 BTU/lb-°F
@Temperature 77.0 °F
Thermal Conductivity 10.0 - 16.0 W/m-K
@Temperature 20.0 °C
69.4 - 111 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Maximum Service Temperature, Air 1150 °C2100 °Flong term
Maximum Service Temperature, Inert 1400 °C2550 °Fcontinuous
 
Component Elements PropertiesMetricEnglishComments
Si3N4 100 %100 %
 
Descriptive Properties
Chemical Resistance - AlkalisFair
Chemical Resistance - Concentrated AcidsFair
Chemical Resistance - Dilute AcidsGood
Chemical Resistance - HalogensGood
Chemical Resistance - MetalsFair

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Silicon Nitride, reaction sintered
Silicon Nitride, Si3N4
Ceradyne Ceralloy® 147-1B Reaction Bonded Silicon Nitride (Si3N4)
Goodfellow Hot Pressed Silicon Nitride Si3N4
Silicon Nitride

CGOODF248 / 197411

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.