MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Bakelite® PF 2874 Phenolic Formaldehyde Resin, Low Shrinkage, Improved Electrical Properties, UL Listed, High Mechanical Strength
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic

Material Notes: Phenolic molding compound, inorganically filled, glass fiber reinforced, increased mechanical strength, increased temperature stability, low water absorption, good dimensional stability, UL listed molding compound 0.75 mm / V-0 (BK).

Applications: Solenoid switch caps, insulating flanges, automotive engine parts, steering housings, electric motor parts, carbon brush holders, medium strength and heat resistant cookware fittings.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.57 g/cc0.0567 lb/in³ISO 1183
Apparent Bulk Density 0.700 g/cc0.0253 lb/in³ISO 60
Linear Mold Shrinkage 0.0025 cm/cm0.0025 in/inCompression Molding. Post Shrinkage = 0.2%.; ISO 2577
 0.0050 cm/cm0.0050 in/inInjection Molding. Post Shrinkage = 0.25%.; ISO 2577
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 350 MPa50800 psiH961/30; ISO 2039/P1
Tensile Strength 65.0 MPa9430 psiISO 527 - 1/2
Tensile Modulus 10.5 GPa1520 ksiISO 527 - 1/2
Flexural Strength 125 MPa18100 psiISO 178
Flexural Modulus 11.0 GPa1600 ksiISO 178
Compressive Strength 220 MPa31900 psiISO 604
Charpy Impact Unnotched 0.950 J/cm²4.52 ft-lb/in²ISO 179-1 eU
Charpy Impact, Notched 0.220 J/cm²1.05 ft-lb/in²ISO 179-1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cm
Surface Resistance 1.00e+11 ohm1.00e+11 ohm
Dielectric Constant 9.0
@Frequency 100 Hz
9.0
@Frequency 100 Hz
Dielectric Strength 25.0 kV/mm
@Thickness 1.00 mm
635 kV/in
@Thickness 0.0394 in
IEC 60243-P1
Dissipation Factor 0.25
@Frequency 100 Hz
0.25
@Frequency 100 Hz
Arc Resistance 130 - 135 sec130 - 135 secASTM D495
Comparative Tracking Index 175 V175 V
Hot Wire Ignition, HWI >= 120 sec
@Thickness 0.750 mm
>= 120 sec
@Thickness 0.0295 in
BK
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness 0.750 mm
>= 120 arcs
@Thickness 0.0295 in
BK
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min
@Thickness 3.00 mm
0.000 - 0.394 in/min
@Thickness 0.118 in
BK
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 170 °C338 °F<20000 hours; IEC 60216-P1
 230 °C446 °F< 50 hours; IEC 60216-P1
Deflection Temperature at 8.0 MPa 155 °C311 °FISO 75-2
UL RTI, Electrical 150 °C
@Thickness 0.750 mm
302 °F
@Thickness 0.0295 in
BK
UL RTI, Mechanical with Impact 150 °C
@Thickness 0.750 mm
302 °F
@Thickness 0.0295 in
BK
UL RTI, Mechanical without Impact 150 °C
@Thickness 0.750 mm
302 °F
@Thickness 0.0295 in
BK
Flammability, UL94 V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
BK
 
Processing PropertiesMetricEnglishComments
Feed Temperature 60.0 - 75.0 °C140 - 167 °FInjection molding
Nozzle Temperature 80.0 - 100 °C176 - 212 °FInjection molding
Melt Temperature 80.0 - 100 °C176 - 212 °FInjection molding
Mold Temperature 160 - 190 °C320 - 374 °FInjection molding
 160 - 190 °C320 - 374 °FCompression molding
Injection Pressure >= 15.0 MPa>= 2180 psiCompression and injection cavity mold pressure
Back Pressure 0.500 - 2.00 MPa72.5 - 290 psiInjection molding
Cure Time 0.167 - 0.333 min0.00278 - 0.00556 hourPer 1 mm of wall thickness, injection molding
 0.333 - 0.667 min0.00556 - 0.0111 hourPer 1 mm of wall thickness, compression molding
 
Descriptive Properties
Chromatic SpectrumAll Colors
Creep Rupture StrengthVery Good
Holding PressureApproximately 40-60% of injection pressure
Media ResistanceVery Good
Thermal ExpansionVery Slight
Water absorption (mg)3024h / 23°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Semitron™ ESd 480 PEEK, static dissipative
Cast Nylons Nycast® Nyloil®-MDX Lubricated Nylon, MoS2 Filled
Bakelite® MP 4165 Melamine Phenolic Resin, Copper Adhesive, Low Shrinkage, High Mechanical Strength
Polikim KESTLUB® Polyamide 6 + Lubricant
Sumitomo Bakelite Sumikon® PM-9750 Type JB Black Phenolic Resol

PBAKE022 / 27056

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.