MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Potassium, K
Categories: Metal; Nonferrous Metal; Pure Element

Material Notes: Physical Form: Soft Silver-White Metal; Cubic

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  0.602 g/cc
@Temperature 1000 °C
0.0217 lb/in³
@Temperature 1830 °F
 0.653 g/cc
@Temperature 800 °C
0.0236 lb/in³
@Temperature 1470 °F
 0.702 g/cc
@Temperature 600 °C
0.0254 lb/in³
@Temperature 1110 °F
 0.751 g/cc
@Temperature 400 °C
0.0271 lb/in³
@Temperature 752 °F
 0.774 g/cc
@Temperature 300 °C
0.0280 lb/in³
@Temperature 572 °F
 0.797 g/cc
@Temperature 200 °C
0.0288 lb/in³
@Temperature 392 °F
 0.820 g/cc
@Temperature 100 °C
0.0296 lb/in³
@Temperature 212 °F
 0.855 g/cc
@Temperature 20.0 °C
0.0309 lb/in³
@Temperature 68.0 °F
 0.873 g/cc
@Temperature -73.0 °C
0.0315 lb/in³
@Temperature -99.4 °F
 0.894 g/cc
@Temperature -173 °C
0.0323 lb/in³
@Temperature -279 °F
 0.909 g/cc
@Temperature -270 °C
0.0328 lb/in³
@Temperature -454 °F
Vapor Pressure  0.150 bar
@Temperature 590 °C
113 torr
@Temperature 1090 °F
 0.500 bar
@Temperature 710 °C
375 torr
@Temperature 1310 °F
 1.00 bar
@Temperature 770 °C
750 torr
@Temperature 1420 °F
 2.00 bar
@Temperature 850 °C
1500 torr
@Temperature 1560 °F
 5.00 bar
@Temperature 950 °C
3750 torr
@Temperature 1740 °F
 10.0 bar
@Temperature 1110 °C
7500 torr
@Temperature 2030 °F
 20.0 bar
@Temperature 1240 °C
15000 torr
@Temperature 2260 °F
 40.0 bar
@Temperature 1420 °C
30000 torr
@Temperature 2590 °F
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 39.098339.09831995
Atomic Number 1919
Thermal Neutron Cross Section 2.7 barns/atom2.7 barns/atom
X-ray Absorption Edge 3.43645 Å3.43645 ÅK
 36.352 Å36.352 ÅLI
 42.02 Å42.02 ÅLII
 42.452 Å42.452 ÅLIII
Critical Temperature 1950 °C3540 °F
Electrode Potential -2.92 V-2.92 V
Electronegativity 0.820.82Pauling
Ionic Radius 1.33 Å1.33 ÅCrystal Ionic Radius for Valence +1
Electrochemical Equivalent 1.46 g/A/h1.46 g/A/h
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.00000649 ohm-cm
@Temperature 0.000 °C
0.00000649 ohm-cm
@Temperature 32.0 °F
 0.00000720 ohm-cm
@Temperature 20.0 °C
0.00000720 ohm-cm
@Temperature 68.0 °F
 0.00000922 ohm-cm
@Temperature 63.0 °C
0.00000922 ohm-cm
@Temperature 145 °F
solid
 0.00001395 ohm-cm
@Temperature 63.0 °C
0.00001395 ohm-cm
@Temperature 145 °F
liquid
 0.00001464 ohm-cm
@Temperature 77.0 °C
0.00001464 ohm-cm
@Temperature 171 °F
liquid
Magnetic Susceptibility 5.2e-75.2e-7cgs/g
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 61.55 J/g26.48 BTU/lb
Heat of Vaporization 2077 J/g893.5 BTU/lb
CTE, linear 83.0 µm/m-°C
@Temperature 20.0 - 100 °C
46.1 µin/in-°F
@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.532 J/g-°C0.127 BTU/lb-°FGas
 0.724 J/g-°C0.173 BTU/lb-°F
Thermal Conductivity 99.2 W/m-K688 BTU-in/hr-ft²-°F
Melting Point 63.25 °C145.9 °F
Boiling Point 759 °C1400 °F
Heat of Formation 0.000 kJ/mol0.000 kJ/molCrystal
 89.0 kJ/mol89.0 kJ/molGas
 
Component Elements PropertiesMetricEnglishComments
Potassium, K 100 %100 %
 
Descriptive Properties
CAS Number7440-09-7

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Silver, Ag
Aluminum, Al
Gold, Au
Americium, Am
Mercury, Hg

AMEK000 / 51

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.