MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Tropical Balsa Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Data is based on small, clear, air-dried samples unless specified.

Key Words: Ochroma lagopus; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.160 g/cc0.00578 lb/in³Air Dry (12-15% Moisture Content)
Cell Length 2.20 mm0.0866 inMature Wood
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 400 N89.9 lb (f)Side
Tensile Strength, Ultimate 1.00 MPa145 psiPerpendicular to Grain
 73.0 MPa10600 psiAxial
Modulus of Rupture 0.0190 GPa2.76 ksiStatic Bending
Flexural Modulus 2.55 - 3.17 GPa370 - 460 ksiStatic Bending
Compressive Strength 1.00 MPa145 psiPerpendicular to Grain
 6.90 - 9.00 MPa1000 - 1310 psiParallel to Grain
Shear Strength 1.10 MPa160 psiOrientation Unknown
Impact 2.22.2J/cm² Toughness
 
Thermal PropertiesMetricEnglishComments
Shrinkage 0.60 %0.60 %Axial; Green to Zero Moisture
 2.4 %2.4 %Radial; Green to Zero Moisture
 4.4 %4.4 %Tangential; Green to Zero Moisture
 7.5 %7.5 %Volumetric; Green to Zero Moisture

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
American Balsa Wood
DIAB ProBalsa® PB Standard Balsa Wood
DIAB ProBalsa® LD7 Light Weight Balsa Wood
Carbon-Core Carbon Balsa Wood
3M Balsa Panels

PTSIA / 71344

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.