MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

3M Balsa Panels
Categories: Wood and Natural Products; Wood

Material Notes: 3M™ Balsa Panels are made of end grain balsa, a highly processed ultra light wood product, imparts impressive strength and stiffness to the sandwich panel. The end grain configuration of balsa provides high resistance to crushing and is very difficult to tear apart. End grain balsa cored panels also have the ability to handle excessive dynamic loads with high resistance to fatigue. The balsa panels end grain orientation gives it exceptional compression and shear properties. As an added benefit, panels providing good thermal and acoustic insulation. Balsa panels are available in 9.5 lb/ft3 density.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.128 - 0.176 g/cc0.00462 - 0.00636 lb/in³
Water Absorption 9.66 %9.66 %
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 13.07 MPa1895 psiASTM C365
Compressive Modulus 4.07 GPa590 ksiASTM C365
Shear Modulus 0.159 GPa23.1 ksiASTM C273
Shear Strength 2.98 MPa432 psiASTM C273

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Carbon-Core Carbon Balsa Wood
DIAB ProBalsa® PB Standard Balsa Wood
3A Composites Core Materials BALTEK® SB.50 Structural End-Grain Balsa
American Balsa Wood
Tropical Balsa Wood

PMM34785 / 169532

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.