MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Hytrel® G3548 NC010 TPC-ET
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE

Material Notes: 35 Shore D Standard Performance Polyester Elastomer with Non-discoloring Stabilizer

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³ISO 1183
Water Absorption 6.9 %
@Time 86400 sec
6.9 %
@Time 24.0 hour
Immersion; Sim. to ISO 62
 12 %
@Thickness 2.00 mm
12 %
@Thickness 0.0787 in
Sim. to ISO 62
Moisture Absorption 0.800 %
@Thickness 2.00 mm
0.800 %
@Thickness 0.0787 in
Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0080 cm/cm0.0080 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/inISO 294-4, 2577
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 190 °C
10 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 242415s; ISO 48-4
Tensile Stress at Strain  1.50 MPa
@Strain 5.0 %
218 psi
@Strain 5.0 %
1BA specimen at 50mm/min; ISO 527-1/-2
 2.50 MPa
@Strain 10 %
363 psi
@Strain 10 %
ISO 527-1/-2
 6.00 MPa
@Strain 50 %
870 psi
@Strain 50 %
ISO 527-1/-2
Flexural Modulus 0.0250 GPa3.63 ksiISO 178
Charpy Impact, Notched  NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
ISO 179/1eA
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eA
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eA
Tear Strength 54.0 kN/m308 pliparallel; ISO 34-1
 70.0 kN/m399 plinormal; ISO 34-1
 
Thermal PropertiesMetricEnglishComments
Melting Point 157 °C315 °F10°C/min; ISO 11357-1/-3
Glass Transition Temp, Tg -45.0 °C-49.0 °F10°C/min; ISO 11357-1/-2
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
IEC 60695-11-10
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
IEC 60695-11-10
Flame Spread 52.0 mm/min
@Thickness 1.00 mm
2.05 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
 
Processing PropertiesMetricEnglishComments
Melt Temperature 170 - 185 °C338 - 365 °FRange, Extrusion
 180 °C356 °FOptimum, Extrusion
 190 °C374 °FOptimum, Injection
 180 - 210 °C356 - 410 °FRange, Injection
Mold Temperature 30.0 - 40.0 °C86.0 - 104 °FInjection
 40.0 °C104 °FOptimum, Injection
Drying Temperature 80.0 °C176 °FExtrusion
 90.0 °C194 °FInjection
Dry Time 2.00 - 3.00 hour2.00 - 3.00 hourExtrusion, Dehumidified Dryer
 2.00 - 3.00 hour2.00 - 3.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.060 %<= 0.060 %Extrusion
 <= 0.080 %<= 0.080 %Injection
 
Descriptive Properties
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
Part Marking Code>TPC-ET<ISO 11469
PolymerTPC
Resin IdentificationTPC-ETISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Hytrel® 3046 NC010 TPC-ET
Celanese Hytrel® 3078 TPC-ET
Toyobo Pelprene™ P-30B Polyester TPE
BASF Ultramid® A3K BK00464 PA66 (Dry)
Celanese Riteflex® 425 TPC, Unfilled

PDSX5196 / 197836

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.