MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Riteflex® 425 TPC, Unfilled
Categories: Polymer; Thermoplastic; Polyester, TP; Polyester Thermoplastic Elastomer

Material Notes: Riteflex 425 is a nominal 25 Shore D thermoplastic polyester elastomer with low modulus and outstanding low temperature impact, and tear resistance.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.012 cm/cm0.012 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.012 cm/cm0.012 in/inISO 294-4
Melt Flow 13 g/10 min
@Load 2.16 kg,
Temperature 190 °C
13 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7979ISO 868
Hardness, Shore D 242415 sec; ISO 868
Tensile Strength at Break 10.0 MPa1450 psi50mm/min; ISO 527-2/1A
Tensile Stress at Strain  1.00 MPa
@Strain 5.0 %
145 psi
@Strain 5.0 %
ISO 527-1/2
 2.00 MPa
@Strain 10 %
290 psi
@Strain 10 %
ISO 527-1/2
 3.00 MPa
@Strain 50 %
435 psi
@Strain 50 %
ISO 727-1/2
 3.00 MPa
@Strain 50 %
435 psi
@Strain 50 %
ISO 527-2/1A
Elongation at Break 750 %750 %50mm/min; ISO 527-2/1A
Flexural Strength 1.00 MPa145 psiISO 178
 1.00 MPa
@Strain 3.5 %
145 psi
@Strain 3.5 %
ISO 178
Flexural Modulus 0.0170 GPa2.47 ksiISO 178
 0.00800 GPa
@Temperature 100 °C
1.16 ksi
@Temperature 212 °F
ISO 178
 0.162 GPa
@Temperature -40.0 °C
23.5 ksi
@Temperature -40.0 °F
ISO 178
Resilience 6565Bayshore, %; ASTM D2632
 6565Bayshore, %
Flex Crack Resistance >= 1.00e+6>= 1.00e+6Ross flex
Izod Impact, Notched (ISO) NBNBISO 180
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 180/1U
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 180/1U
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 180/1A
Charpy Impact Unnotched NBNBISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched NBNBISO 179/1eA
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eA
Tear Strength 61.0 kN/m348 pliISO 34-1
 62.0 kN/m354 pliISO 34-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+14 ohm-cm2.00e+14 ohm-cmIEC 60093
Surface Resistance 2.00e+14 ohm2.00e+14 ohmIEC 60093
Dielectric Constant 5.1
@Frequency 1e+6 Hz
5.1
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 24.0 kV/mm610 kV/inIEC 60243-1
Comparative Tracking Index >= 600 V>= 600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 250 µm/m-°C139 µin/in-°FISO 11359-2
Melting Point 155 °C311 °F10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 0.46 MPa (66 psi) 42.0 °C108 °FISO 75-1, -2
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 20.0 - 55.0 °C68.0 - 131 °Fcavity
 170 - 190 °C338 - 374 °Fhot runner
Feed Temperature 155 - 170 °C311 - 338 °F
Zone 1 155 - 170 °C311 - 338 °F
Zone 2 170 - 180 °C338 - 356 °F
Zone 3 170 - 180 °C338 - 356 °F
Zone 4 170 - 180 °C338 - 356 °F
Die Temperature 170 - 190 °C338 - 374 °F
Melt Temperature 170 - 190 °C338 - 374 °F
Drying Temperature 100 - 110 °C212 - 230 °F
Dry Time 4.00 hour4.00 hour
Moisture Content <= 0.050 %<= 0.050 %
 
Descriptive Properties
Injection moldingYes
Injection speedmedium-fast
Processing typeInj/Blow/Ext

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Riteflex® 435 TPC, Unfilled
Celanese Riteflex® 265B TPC
Celanese Riteflex® 640A TPC, Unfilled
Celanese Riteflex® 447 TPC, Unfilled
Celanese Hytrel® G3548 NC010 TPC-ET

PHCQ447 / 178902

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.