MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Riteflex® 425 TPC, Unfilled
Categories: Polymer; Thermoplastic; Polyester, TP; Polyester Thermoplastic Elastomer

Material Notes: Riteflex 425 is a nominal 25 Shore D thermoplastic polyester elastomer with low modulus and outstanding low temperature impact, and tear resistance.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.06 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.012 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.012 cm/cmISO 294-4
Melt Flow 13 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 79ISO 868
Hardness, Shore D 2415 sec; ISO 868
Tensile Strength at Break 10.0 MPa50mm/min; ISO 527-2/1A
Tensile Stress at Strain 1.00 MPa
@Strain 5.0 %
ISO 527-1/2
 2.00 MPa
@Strain 10 %
ISO 527-1/2
 3.00 MPa
@Strain 50 %
ISO 727-1/2
 3.00 MPa
@Strain 50 %
ISO 527-2/1A
Elongation at Break 750 %50mm/min; ISO 527-2/1A
Flexural Strength 1.00 MPaISO 178
 1.00 MPa
@Strain 3.5 %
ISO 178
Flexural Modulus 17.0 MPaISO 178
 8.00 MPa
@Temperature 100 °C
ISO 178
 162 MPa
@Temperature -40.0 °C
ISO 178
Resilience 65Bayshore, %; ASTM D2632
 65Bayshore, %
Flex Crack Resistance >= 1.00e+6Ross flex
Izod Impact, Notched (ISO) NBISO 180
 NB
@Temperature -30.0 °C
ISO 180/1U
 NB
@Temperature 23.0 °C
ISO 180/1U
 NB
@Temperature -30.0 °C
ISO 180/1A
Charpy Impact Unnotched NBISO 179/1eU
 NB
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched NBISO 179/1eA
 NB
@Temperature -30.0 °C
ISO 179/1eA
Tear Strength 61.0 kN/mISO 34-1
 62.0 kN/mISO 34-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.00e+14 ohm-cmIEC 60093
Surface Resistance 2.00e+14 ohmIEC 60093
Dielectric Constant 5.1
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 24.0 kV/mmIEC 60243-1
Comparative Tracking Index >= 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 250 µm/m-°CISO 11359-2
Melting Point 155 °C10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 0.46 MPa (66 psi) 42.0 °CISO 75-1, -2
Flammability, UL94 HB
@Thickness 1.50 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 20.0 - 55.0 °Ccavity
 170 - 190 °Chot runner
Feed Temperature 155 - 170 °C
Zone 1 155 - 170 °C
Zone 2 170 - 180 °C
Zone 3 170 - 180 °C
Zone 4 170 - 180 °C
Die Temperature 170 - 190 °C
Melt Temperature 170 - 190 °C
Drying Temperature 100 - 110 °C
Dry Time 4.00 hour
Moisture Content <= 0.050 %
 
Descriptive Properties
Injection moldingYes
Injection speedmedium-fast
Processing typeInj/Blow/Ext

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Riteflex® 435 TPC, Unfilled
Celanese Riteflex® 265B TPC
Celanese Riteflex® 640A TPC, Unfilled
Celanese Riteflex® 447 TPC, Unfilled
Celanese Hytrel® G3548 NC010 TPC-ET

PHCQ447 / 178902

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.