MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Dyneon™ TF 2029 PTFE  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes:
  • Processable by standard paste extrusion methods
  • Designed for low reduction ratios
  • Can be processed at a high stretch ratios
  • Recommended for apes requiring high mechanical strength, such as electrical tape for wrapped insulation or flat cables
  • Recommended for yarn applications, such as sewing or weaving yard for filter and sealing materials or dental floss
  • Can be used to extrude pipe liners requiring green strength higher that TF 2025

Information provided by Dyneon, A 3M Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.480 g/cc0.0173 lb/in³ISO 12086
Density 2.15 g/cc0.0777 lb/in³ISO 12086
Particle Size 500 µm500 µmaverage; ISO 12086
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 28.0 MPa4060 psiISO 12086
Elongation at Break 340 %340 %ISO 12086
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+19 ohm-cm1.00e+19 ohm-cmIEC 60093
Surface Resistance 1.00e+18 ohm1.00e+18 ohmIEC 60093
 
Descriptive Properties
Extrusion Pressure50 MPareduction ratio 400, ASTM D4894
Reduction Ratio Range5-100:1Dyneon Method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
TriStar TriSteel PT Metal Backed PTFE Bearing System
TriStar TriSteel PE Metal Backed PTFE Bearing System
TriStar TriSteel AC Metal Backed PTFE Bearing System
Overview of materials for Polytetrafluoroethylene (PTFE), Molded
Honeywell ACumist® 3105B PE homopolymer, PTFE-modified

PDYNE041 / 34849

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.