MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Saint-Gobain Tygon® 2375 Ultra Chemical Resistant Tubing Formulation
Categories: Polymer; Thermoplastic

Material Notes: Tygon® Ultra Chemical Resistant Tubing offers a combination of chemical resistance, clarity and flexibility. Tygon® 2375 replaces 2075.

Tygon® Ultra Chemical Resistant Tubing is virtually unaffected by acids, bases, ketones, salts and alcohols, fitting the requirements of many applications from battery acid filling to hazardous material handling. It's entirely plasticizer-free, eliminating fluid contamination and the premature embrittlement and cracking common with many flexible tubings. Its exceptionally smooth inner surface inhibits particulate buildup and reduces the potential for contamination.

Applications

  • Battery acid filling
  • Clean and degreaser transfer systems
  • Fine and specialty chemical production
  • Hazardous materials handling
  • Ink and printing fluid dispensing
  • Paint and solvent production
  • Power generation sampling and drain lines
  • X-ray processing

Features and Benefits

  • Resistant to highly aggressive chemicals
  • Plasticizer-free -- minimizes risk of fluid contamination
  • Exceptionally smooth inner surface inhibits particulate buildup
  • Low sorption maintains fluid integrity
  • Meets USP Class VI criteria

Regulatory Information: This product complies with FDA and NSF 51 criteria.

Unless otherwise noted, all tests were conducted at room temperature. Values shown were determined on 1.9 mm thick extruded strip or 1.9 mm thick molded ASTM plaques or molded ASTM durometer buttons.

Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.900 g/cc0.900 g/ccASTM D792
Water Absorption 0.040 %
@Temperature 22.8 °C,
Time 86400 sec
0.040 %
@Temperature 73.0 °F,
Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 75
@Time 15.0 sec
75
@Time 0.00417 hour
ASTM D2240
Tensile Strength 13.1 MPa1900 psiASTM D412
Elongation at Break 850 %850 %ASTM D412
100% Modulus 2.93 MPa
@Strain 100 %
425 psi
@Strain 100 %
ASTM D412
Tear Strength 42.1 kN/m240 pliASTM D1004
Compression Set 100 %
@Temperature 70.0 °C,
Time 79200 sec
100 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395 Method B
Tensile Set 300 %
@Strain 75 %
300 %
@Strain 75 %
ASTM D412
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 54.4 °C130 °F
Brittleness Temperature -75.0 °C-103 °FASTM D746
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %Clear, but value not quantified
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
NSF YesYes
USP Class VI YesYes
 
Descriptive Properties
ColorClear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Saint-Gobain Tygon® 2001 Plasticizer Free Tubing Formulation
Saint-Gobain Tygon® Chemfluor® Convoflex™ Spiral Designed Tubing Aids in Self-flushing and Cleaning
Saint-Gobain Tygon® A-60-N Drinking Water Tubing Formulation
Saint-Gobain Tygon® A-60-F I.B. Pressure Tubing Formulation for CIP and SIP cleaning and sterilization systems
Saint-Gobain Tygon® Tygoprene® XL-60 Pump Tubing Formulation

PSTGQ912 / 160408

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.