MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay SIPOMER® PAM-100 Phosphate Esters of Polyethylene Glycol Monomethacrylate
Categories: Fluid

Material Notes: Description: Sipomer PAM-100 incorporated into acrylic or styrene acrylic latex systems improves adhesion to metallic substrates and glass. Sipomer PAM-100 also enhances properties such as freeze/thaw stability, mechanical stability, and gloss. This monomer has been used mainly in Specialty Purpose Coatings, including industrial maintenance, OEM coil, light industrial, as well as high performance structural adhesives.

Chemical Name: PHOSPHATE ESTERS OF POLYETHYLENE GLYCOL MONOMETHACRYLATE

Available in: Asia Pacific, Europe, Latin America and North America

Applications: SIPOMER© PAM-100 incorporated into acrylic latex systems improves adhesion to metallic substrates and glass. SIPOMER© PAM-100 also enhances properties such as freeze/thaw stability, mechanical stability, and gloss. This monomer has been used mainly in Specialty Purpose Coatings, including industrial maintenance, OEM coil, light industrial, as well as high performance structural adhesives.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
pH 1.8 - 1.91.8 - 1.91% aqueous solution
Viscosity 1700 cP1700 cP
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 131.5131.5[mg KOH/g], #1
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 20.0 °C68.0 °Ffor homopolymer
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 1.0 %<= 1.0 %Karl fisher; RP-0327
 
Descriptive Properties
AppearanceDark Brown, Clean Viscous LiquidRP-0064
CompositionActive Matter96-97%
 MEHQ2500-5500 ppm, RP-1408
OdorMild Acrylic Odor

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay SIPOMER® PAM-4000 Ethylmethacrylate Phosphate; Alkyl Methacrylate Phosphate
Evonik MHOROMER® D 1133 Polyethylene Glycol 200 Dimethacrylate
DSM Biomedical PurSil® 35 Thermoplastic Silicone Polyether Polyurethane (TSPU)
Solvay SIPOMER® PAM-200 Phosphate Esters of Ppg Monomethacrylate
DSM Biomedical PurSil® 20 Thermoplastic Silicone Polyether Polyurethane (TSPU)

WRHOD505 / 137736

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.