MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik MHOROMER® D 1133 Polyethylene Glycol 200 Dimethacrylate  (discontinued **)
Categories: Fluid

Material Notes: Application: Crosslinking agent for free radical polymerization. Constituent of reactive adhesives.

Appearance: Clear, colorless to yellowish liquid

Odor: Weak, ester-like

CAS: 25852-47-5

Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm GmbH, although this trade name was disontinued prior to the sale.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.083 g/cc0.03913 lb/in³
Viscosity 17 cP
@Temperature 20.0 °C
17 cP
@Temperature 68.0 °F
Molecular Weight 336 g/mol336 g/mol
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 0.10<= 0.10Rohm Method: M4 (acid-base titr., MAAC)
 
Thermal PropertiesMetricEnglishComments
Boiling Point 200 °C
@Pressure 0.000130 MPa
392 °F
@Pressure 0.0189 psi
Flash Point 150 °C302 °FDIN-EN 22719
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.463
@Temperature 20.0 °C
1.463
@Temperature 68.0 °F
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 0.30 %<= 0.30 %Rohm Method: M3 (according to K. Fischer)
 
Descriptive Properties
Colormax. 100Rohm Method: M5 (Pt-Co)
Degree of Purity (%)min. 95Rohm Method: M2-114 (GC)
MEHQ180-220ppm, Rohm Method: M1-1 (HPLC), MEHQ
MMA content (%)max. 0.15Rohm Method: M2-114 (GC)
Reactive Ester Content (%)min. 98Rohm Method: M2-114 (GC)

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay SIPOMER® PAM-100 Phosphate Esters of Polyethylene Glycol Monomethacrylate
DSM Biomedical PurSil® 20 Thermoplastic Silicone Polyether Polyurethane (TSPU)
Eastman DuraStar DS1000 Polymer, Natural
DSM Biomedical PurSil® 35 Thermoplastic Silicone Polyether Polyurethane (TSPU)
Polyglycolic Acid (PGA)

PCYR00101 / 101090

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.