MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Asahi Kasei Thermylene® P-20TC-5100 20% Talc Filled, Heat Stabilized Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Talc Filler

Material Notes: Information provided by Asahi Thermofil, now Asahi Kasei North America.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/ccASTM D792
Linear Mold Shrinkage 0.014 cm/cm0.014 in/inASTM D955
Melt Flow 6.0 g/10 min6.0 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9292ASTM D785
Tensile Strength, Yield 32.4 MPa4700 psiASTM D638
Elongation at Yield 30 %30 %ASTM D638
Flexural Strength 49.6 MPa7200 psiASTM D790
Flexural Modulus 2.14 GPa310 ksiASTM D790
Izod Impact, Notched 0.267 J/cm0.500 ft-lb/inASTM D256
Izod Impact, Unnotched 4.81 J/cm9.00 ft-lb/inASTM D4812
 
Thermal PropertiesMetricEnglishComments
CTE, linear 59.4 µm/m-°C
@Temperature 20.0 °C
33.0 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 130 °C266 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C176 °FASTM D648
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
Flame Spread 15 mm/min0.60 in/minHorizontal Burn Rate; FMVSS302

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Gromax PBT 4130-104D 30% Glass Fiber Filled
Mytex Polymers AS171L-02US Polypropylene, 13% Talc Filled
Trinseo PULSE™ EXT 100 PC/ABS Engineering Resin
Asahi Kasei Thermylene® P6-30FG-1804 30% Glass Fiber Reinforced, Heat and UV Polypropylene
Asahi Kasei Thermylene® P-20TC-5100 Chemically Coupled Polypropylene Compound, 20% Talc Filled Polypropylene

PTHER045 / 70144

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.