MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Trinseo PULSE™ EXT 100 PC/ABS Engineering Resin
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: PULSE™ EXT 100 engineering resin has been designed to provide excellent processability, high heat resistance and high impact strength at room and low temperatures. PULSE EXT 100 engineering resin has been used in automotive plated and painted exterior trim applications.

Applications:

  • Front Grilles
  • Wheel Covers and Center Caps
  • Decorative Trim
  • Name Plates and Badges
Automotive Specifications:
  • CHRYSLER MS-DB-195 CPN2967
  • CHRYSLER MS-DB-195 CPN3094
  • CHRYSLER MS-DB-195 CPN3159
  • GM GMP.ABS+PC.010
  • TOYOTA TSM 5526G-1

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ASTM D792
Linear Mold Shrinkage, Flow 0.0060 cm/cm0.0060 in/inASTM D955
Melt Flow 1.3 g/10 min
@Load 3.80 kg,
Temperature 230 °C
1.3 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 51.7 MPa7500 psiType I, 51 mm/min; ASTM D638
Elongation at Break 80 %80 %Type I, 51 mm/min; ASTM D638
Flexural Yield Strength 82.7 MPa12000 psiASTM D790
Flexural Modulus 2.24 GPa325 ksiASTM D790
Izod Impact, Notched  4.80 J/cm
@Thickness 3.20 mm,
Temperature -29.0 °C
8.99 ft-lb/in
@Thickness 0.126 in,
Temperature -20.2 °F
0.25 mm Notch Depth; ASTM D256
 6.40 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
12.0 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
0.25 mm Notch Depth; ASTM D256
Dart Drop, Total Energy  54.2 J
@Thickness 3.20 mm,
Temperature 23.0 °C
40.0 ft-lb
@Thickness 0.126 in,
Temperature 73.4 °F
3.39 m/sec; ASTM D3763
 59.9 J
@Thickness 3.20 mm,
Temperature -29.0 °C
44.2 ft-lb
@Thickness 0.126 in,
Temperature -20.2 °F
3.39 m/sec; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 72.0 µm/m-°C
@Temperature -40.0 - 82.0 °C
40.0 µin/in-°F
@Temperature -40.0 - 180 °F
ASTM D696
Specific Heat Capacity 1.98 J/g-°C0.473 BTU/lb-°FMelt; ASTM C351
Thermal Conductivity 0.260 W/m-K1.80 BTU-in/hr-ft²-°FMelt; ASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 124 °C
@Thickness 3.20 mm
255 °F
@Thickness 0.126 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 107 °C
@Thickness 3.20 mm
225 °F
@Thickness 0.126 in
Unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Ejection Temperature 138 °C280 °F
 
Descriptive Properties
No Flow Temperature160°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution Lustran® 433 Acrylonitrile Butadiene Styrene (ABS)
LG Chemical LUPOY HI5002A PC/ABS, High Impact
INEOS Styrolution Terluran® GP-35 ABS
Lotte Advanced Materials Infino® WP-1041 PC/ABS, Unreinforced Metal Plating Grade
Asahi Kasei Thermylene® P-20TC-5100 20% Talc Filled, Heat Stabilized Polypropylene

PDWST083 / 142292

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.