MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Fluorocarbon ETFE/ECTFE, Molded/Extruded
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE; Fluorocarbon ETFE/ECTFE, Molded/Extruded

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE/ECTFE, Molded/Extruded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.18 - 1.88 g/cc0.0427 - 0.0679 lb/in³Average value: 1.73 g/cc Grade Count:35
Water Absorption 0.00700 - 0.0300 %0.00700 - 0.0300 %Average value: 0.0206 % Grade Count:13
Water Absorption at Saturation 0.0100 - 0.100 %0.0100 - 0.100 %Average value: 0.0775 % Grade Count:4
Particle Size 100 - 500 µm100 - 500 µmAverage value: 288 µm Grade Count:6
Water Vapor Transmission 12.92 - 12.92 g/m²/day
@Temperature 37.8 - 37.8 °C
0.8320 - 0.8320 g/100 in²/day
@Temperature 100 - 100 °F
Average value: 12.9 g/m²/day Grade Count:1
Thickness 1.00 - 2000 microns0.0394 - 78.7 milAverage value: 872 microns Grade Count:12
Linear Mold Shrinkage 0.0180 - 0.0250 cm/cm0.0180 - 0.0250 in/inAverage value: 0.0200 cm/cm Grade Count:7
Melt Flow 1.00 - 60.0 g/10 min1.00 - 60.0 g/10 minAverage value: 14.4 g/10 min Grade Count:29
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 90.0 - 94.090.0 - 94.0Average value: 91.3 Grade Count:3
Hardness, Shore D 62.0 - 75.062.0 - 75.0Average value: 69.9 Grade Count:15
Tensile Strength, Ultimate 20.0 - 59.0 MPa2900 - 8560 psiAverage value: 41.5 MPa Grade Count:32
 4.55 - 50.0 MPa
@Temperature 40.0 - 200 °C
660 - 7250 psi
@Temperature 104 - 392 °F
Average value: 23.2 MPa Grade Count:5
Tensile Strength, Yield 5.00 - 30.0 MPa725 - 4350 psiAverage value: 17.0 MPa Grade Count:7
Elongation at Break 50.0 - 950 %50.0 - 950 %Average value: 444 % Grade Count:34
 410 - 620 %
@Temperature 200 - 200 °C
410 - 620 %
@Temperature 392 - 392 °F
Average value: 528 % Grade Count:5
Elongation at Yield 4.00 - 5.00 %4.00 - 5.00 %Average value: 4.67 % Grade Count:3
Modulus of Elasticity 0.500 - 1.66 GPa72.5 - 241 ksiAverage value: 1.48 GPa Grade Count:5
Flexural Yield Strength 24.0 - 48.3 MPa3480 - 7000 psiAverage value: 34.9 MPa Grade Count:9
 5.00 - 20.0 MPa
@Temperature 35.0 - 150 °C
725 - 2900 psi
@Temperature 95.0 - 302 °F
Average value: 12.5 MPa Grade Count:5
Flexural Modulus 0.860 - 1.69 GPa125 - 245 ksiAverage value: 1.11 GPa Grade Count:16
 0.100 - 0.900 GPa
@Temperature 30.0 - 120 °C
14.5 - 131 ksi
@Temperature 86.0 - 248 °F
Average value: 0.369 GPa Grade Count:5
Compressive Yield Strength 8.00 - 38.0 MPa1160 - 5510 psiAverage value: 17.4 MPa Grade Count:11
Flex Crack Resistance 8500 - 6000008500 - 600000Average value: 65500 Grade Count:19
Izod Impact, Notched 100 - 5340 J/cm187 - 10000 ft-lb/inGrade Count:14
 2.10 - 2.10 J/cm
@Temperature -40.0 - -40.0 °C
3.93 - 3.93 ft-lb/in
@Temperature -40.0 - -40.0 °F
Average value: 2.10 J/cm Grade Count:2
 2.10 - 2.10 J/cm
@Thickness 3.20 - 3.20 mm
3.93 - 3.93 ft-lb/in
@Thickness 0.126 - 0.126 in
Average value: 2.10 J/cm Grade Count:2
Coefficient of Friction 0.0300 - 1.600.0300 - 1.60Average value: 0.380 Grade Count:10
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+14 - 1.00e+17 ohm-cm1.00e+14 - 1.00e+17 ohm-cmAverage value: 7.88e+16 ohm-cm Grade Count:23
Surface Resistance 7000 - 1.00e+15 ohm7000 - 1.00e+15 ohmAverage value: 5.58e+14 ohm Grade Count:9
Dielectric Constant 2.50 - 2.602.50 - 2.60Average value: 2.59 Grade Count:24
Dielectric Strength 14.0 - 197 kV/mm356 - 5000 kV/inAverage value: 53.0 kV/mm Grade Count:25
Dissipation Factor 0.000600 - 0.01000.000600 - 0.0100Average value: 0.00409 Grade Count:16
Arc Resistance 120 - 122 sec120 - 122 secAverage value: 122 sec Grade Count:6
 
Thermal PropertiesMetricEnglishComments
CTE, linear 9.00 - 140 µm/m-°C5.00 - 77.8 µin/in-°FAverage value: 103 µm/m-°C Grade Count:14
Specific Heat Capacity 0.962 - 1.26 J/g-°C0.230 - 0.301 BTU/lb-°FAverage value: 1.18 J/g-°C Grade Count:8
Thermal Conductivity 0.150 - 0.216 W/m-K1.04 - 1.50 BTU-in/hr-ft²-°FAverage value: 0.179 W/m-K Grade Count:3
 0.150 - 0.150 W/m-K
@Temperature 40.0 - 40.0 °C
1.04 - 1.04 BTU-in/hr-ft²-°F
@Temperature 104 - 104 °F
Average value: 0.150 W/m-K Grade Count:2
Melting Point 180 - 280 °C356 - 536 °FAverage value: 246 °C Grade Count:33
Maximum Service Temperature, Air 149 - 180 °C300 - 356 °FAverage value: 151 °C Grade Count:32
Deflection Temperature at 0.46 MPa (66 psi) 82.0 - 115 °C180 - 239 °FAverage value: 94.6 °C Grade Count:7
Deflection Temperature at 1.8 MPa (264 psi) 62.0 - 85.0 °C144 - 185 °FAverage value: 68.3 °C Grade Count:9
Brittleness Temperature -125 - -76.0 °C-193 - -105 °FAverage value: -111 °C Grade Count:7
Flammability, UL94 V-0V-0Grade Count:14
Oxygen Index 30.0 - 52.0 %30.0 - 52.0 %Average value: 36.2 % Grade Count:22
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 290 - 320 °C554 - 608 °FAverage value: 305 °C Grade Count:13
Melt Temperature 260 - 300 °C500 - 572 °FAverage value: 280 °C Grade Count:13
Mold Temperature 60.0 - 120 °C140 - 248 °FAverage value: 90.0 °C Grade Count:13
Injection Velocity 1.00 - 15.0 mm/sec0.0394 - 0.591 in/secAverage value: 8.00 mm/sec Grade Count:13
Injection Pressure 50.0 - 120 MPa7250 - 17400 psiAverage value: 85.0 MPa Grade Count:13

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded
Overview of materials for Fluorinated Ethylene Propylene (FEP), Molded/Extruded
3M Scotch® FP-301 Heat Shrink Tubing
Overview of materials for High Density Polyethylene (HDPE), Extruded
Overview of materials for ECTFE Fluoropolymer

O1936 / 77921

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.