MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Buckeye Polymers BP RPP 2012 T NAT Polypropylene, Calcium Carbonate Filled
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Calcium Carbonate (CaCO3) Filler

Material Notes: Product Information: Calcium Carbonate Filled PP Grades have a high impact toughness, moderate increased stiffness, and excel in high gloss applications. Our BP RPP C series product line ranges from 10-50% in filler levels. These materials can be customized through the addition of UV packages, custom matching, and processing additives.

    Product Features:
  • Can be UV stabilized for increased resistance
  • Industrial, outdoor furniture, and window trim
  • Processing Method: Injection Molding

    Information Provided by Buckeye Polymers, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 6.0 - 15 g/10 min6.0 - 15 g/10 minASTM D1238
Ash 18 - 23 %18 - 23 %ASTM D5630
 
Mechanical PropertiesMetricEnglishComments
Flexural Modulus >= 1.63 GPa>= 236 ksiASTM D790
Izod Impact, Notched >= 0.534 J/cm>= 1.00 ft-lb/inASTM D256

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bamberger Polymers Bapolene® 5063C Polypropylene, Injection Grade
Buckeye Polymers BP RPP 3005 GR BLK Polypropylene, Glass Filled
Buckeye Polymers BP RPP 1310 T NAT Polypropylene, Talc Filled
Buckeye Polymers BP RPP 1012 T BLK Polypropylene, Talc Filled
Braskem RP 141 Injection Molding Polypropylene

PBUCK032 / 104499

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.