MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Riteflex® 647 Thermoplastic Polyester Elastomer (TPE)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE; Polyester, TP; Polyester Thermoplastic Elastomer

Material Notes: Description: Riteflex 647 is a thermoplastic elastomer with a 47 Shore D hardness and a 21,300psi flexural modulus

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0423 lb/in³ISO 1183 & ASTM D792
Water Absorption 0.50 %0.50 %ASTM D570
Linear Mold Shrinkage 0.013 cm/cm0.013 in/inASTM D955
Melt Flow 10 g/10 min10 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4747ASTM D2240 & ISO 868
Tensile Strength at Break 22.5 MPa3260 psiASTM D638
Elongation at Break 470 %470 %ASTM D638
Tensile Modulus 0.125 GPa18.1 ksi1 mm/min; ISO 527-2/1A
 0.151 GPa21.9 ksiASTM D638
50% Modulus 12.0 MPa
@Strain 50 %
12.0 MPa
@Strain 50 %
ISO 527-2/1A
Flexural Modulus 0.125 GPa18.1 ksiISO 178
 0.147 GPa21.3 ksiASTM D790
 0.371 GPa
@Temperature -40.0 °C
53.8 ksi
@Temperature -40.0 °F
ASTM D790
Izod Impact, Notched NBNBASTM D256
 2.72 J/cm
@Temperature -40.0 °C
5.10 ft-lb/in
@Temperature -40.0 °F
ASTM D256
Charpy Impact Unnotched NBNBISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched NBNBISO 179/1eA
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eA
Tear Strength 188.4 kN/m1075 pliASTM D624
 195 kN/m1110 pliASTM D1004
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 4.00e+14 ohm-cm4.00e+14 ohm-cmASTM D257
Dielectric Strength 12.2 kV/mm310 kV/inShort Term; ASTM D149
 13.0 kV/mm330 kV/inIEC 60243-1
Dissipation Factor 0.040
@Frequency 1e+6 Hz
0.040
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index >= 600 V>= 600 VASTM D3638 & IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 200 µm/m-°C
@Temperature 20.0 °C
111 µin/in-°F
@Temperature 68.0 °F
ISO 11359-2
Melting Point 187 °C369 °FISO 11357-1,2,3
 190 °C374 °FASTM D3419
Deflection Temperature at 0.46 MPa (66 psi) 62.0 °C144 °FISO 75-1, -2
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 185 - 200 °C365 - 392 °F
Middle Barrel Temperature 200 - 210 °C392 - 410 °F
Front Barrel Temperature 200 - 215 °C392 - 419 °F
Nozzle Temperature 200 - 215 °C392 - 419 °F
Melt Temperature 200 - 215 °C392 - 419 °F
Mold Temperature 20.0 - 55.0 °C68.0 - 131 °F
Injection Pressure 82.7 MPa12000 psi
Back Pressure 0.000 - 0.345 MPa0.000 - 50.0 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Riteflex® 635 Thermoplastic Polyester Elastomer (TPE)
Celanese Riteflex® 655 Thermoplastic Polyester Elastomer (TPE)
Eastman Neostar FN005 Elastomer
Envalior Arnitel® EL550 Polyether Ester Elastomer (European and Asian Grade)
Envalior Arnitel® PL461 TPC-ET, Injection Molding

PHCW59 / 46000

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.