MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Scotchkote™ 412 Fusion Bonded Epoxy Coating
Categories: Polymer; Thermoset; Epoxy

Material Notes: 3M Scotchkote Fusion Bonded Epoxy Coating 413 is a one-part, heat curable, thermosetting epoxy coating designed for corrosion protection of reinforcing steel. The epoxy is applied to preheated steel as a dry powder which melts and cures to a uniform coating thickness. This bonding process provides excellent adhesion and coverage on concrete reinforcing bar, wire fabric, piling, tensioning hardware and other steel member of any size or shape. Scotchkote 413 is resistant to corrosive agents such as deicing salts, airborne slat spray, sea water, harsh chemicals, acid rain, carbonation, contaminated aggregate and concrete additives.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.21 g/cc0.0437 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Knoop >= 16>= 16
Impact Test 9.04 J6.67 ft-lbASTM A775
 18.1 J13.3 ft-lb0.32cm x 7.6cm x 7.6cm steel panel, 1.6cm radius tup; ASTM G14
Penetration 0.00
@Temperature -40.0 - 116 °C
0.00
@Temperature -40.0 - 241 °F
ASTM G17
Abrasion 1717[mg] CS-17, 1000 cycles, 1000g; ASTM D775
 
Processing PropertiesMetricEnglishComments
Gel Time  0.066666 - Error in fixSigDigits: @digits must be between 1 and 12. @digits is: 15 min
@Temperature 232 °C
0.066666 - Error in fixSigDigits: @digits must be between 1 and 12. @digits is: 15 min
@Temperature 450 °F
 0.100 - 0.150 min
@Temperature 204 °C
0.100 - 0.150 min
@Temperature 399 °F
 
Descriptive Properties
AppearanceGreen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Scotchkote™ 206N XTRA LG Fusion Bonded Epoxy Coating
3M Scotchkote™ 426 Fusion Bonded Epoxy Coating
3M Scotchkote™ 412 Spray Grade Fusion Bonded Epoxy Coating
3M Scotchkote™ 206N Fusion Bonded Epoxy Coating (Fluid Bed Grade)

PMM35344 / 170091

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.