MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical Phenol
Categories: Fluid

Material Notes: Structure & Characteristics: C6H5OH. Phenol is a white crystalline solid with a distinct smell

Uses: Raw material of phenolic resins, dye stuffs, synthetic fibers, herbicides, photo material, aromatic essences, etc. Moreover, it is also used as disinfectants and sterilizers. We also use phenol as the base material for our BPA

CAS: 108-95-2

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity >= 1.0009 g/cc>= 1.0009 g/cc1% aq' sol
Viscosity  1.09 cP
@Temperature 100 °C
1.09 cP
@Temperature 212 °F
 1.56 cP
@Temperature 80.0 °C
1.56 cP
@Temperature 176 °F
 2.47 cP
@Temperature 60.0 °C
2.47 cP
@Temperature 140 °F
 3.8 cP
@Temperature 45.0 °C
3.8 cP
@Temperature 113 °F
Molecular Weight 94.11 g/mol94.11 g/mol
Vapor Pressure  0.000280 bar
@Temperature 25.0 °C
0.210 torr
@Temperature 77.0 °F
 0.00349 bar
@Temperature 50.0 °C
2.62 torr
@Temperature 122 °F
 0.0540 bar
@Temperature 100 °C
40.5 torr
@Temperature 212 °F
 0.52999 bar
@Temperature 160 °C
397.53 torr
@Temperature 320 °F
 
Chemical PropertiesMetricEnglishComments
Critical Temperature 419 °C786 °F
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 122.3 J/g52.59 BTU/lb
Heat of Vaporization 489 J/g210 BTU/lb@ B.P.
Specific Heat Capacity 1.28 J/g-°C0.306 BTU/lb-°F
Melting Point 37.9 °C100 °F
Boiling Point 181.8 °C359.2 °F
Flash Point 79.0 °C174 °FCC
 85.0 °C185 °FTOC
Ignition Temperature >= 715 °C>= 1320 °F
 716 °C1320 °FAutoignition
 
Descriptive Properties
Color<10 Pt/CoMolten
 Clear
ComponentsWater Content<300 ppm
Explosion limit0.015
Heat of combustion-7.754 cal/g
Purity>99.95%
Solidification>40.8°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Huntsman Araldite PY 307-1 Epoxy Phenol Novolac
Kazanorgsintez Phenol Resin
Mitsui MILEX™ XL-225MB Phenol Aralkyl Resin, Standard Grade
Sumitomo Bakelite Durez® 32324 Alkyl Phenol Resol
JIS S45C Steel, Normalized

PLAY765 / 148775

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.