MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kazanorgsintez Phenol Resin
Categories: Fluid

Material Notes: Phenol resin is a by-product of phenol and acetone production by the cumene method.

Application: Phenol resin is used in the production of phenol-formaldehyde resins and commercial hydrocarbon as a raw material component and also as a binding agent in by-product coke manufacture.

Information Provided by Kazanorgsintez

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 62.0 °C>= 144 °Fin a closed crucible
 
Component Elements PropertiesMetricEnglishComments
Free Water <= 0.20 %<= 0.20 %Grade B
 
Descriptive Properties
Amount of impurities [pcs]2.5Mechanical impurities
AppearanceBrown colored viscous liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical Phenol
Haveg 41NA Phenolic; Silicate Filled
Huntsman Araldite PY 307-1 Epoxy Phenol Novolac
Mitsui MILEX™ XL-225MB Phenol Aralkyl Resin, Standard Grade
Sumitomo Bakelite Durez® 32324 Alkyl Phenol Resol

PKAZAN182 / 127501

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.