MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Abatron AboWeld/AboCure 7812-2 Thixotropic Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: AboWeld/AboCure 7812-2 is an underwater and cold-weather structural and dielectric adhesive paste. It is a 2-component thixotropic epoxy compound for dry, wet, and cold applications. It has many special characteristics: Lighter Consistency is not just for easy cold mixing, but for the blending with sand, fibers, steel-wool, cloth, bags and other help skin-divers prefer; Fast Reaction Speed compensates for freezing weather slow reactivity, as needed in most underwater applications; the Induction Period normal epoxies require is eliminated to facilitate proper reaction in adverse conditions; where needed, a Pressure-Relief Pipe Section can be inserted through a 7812-2 patch to keep water flowing while the 6712-2 hardens, and then later the pipe can be capped or stuffed with a plug + 7812-2, etc. Suggested Uses: Structural ? Patching, Bonding, Resurfacing, and Filling on virtually all rigid surfaces like concrete, masonry, metal, ceramics, glass, fiberglass, in factories, in industrial, construction and marine applications, under water and under snow, as well as in normal conditions. It can be used alone or mixed with sand, fabric, fibers, steel-wool and other fillers to repair, bond, resurface or fill above and below water, in warm or freezing weather for the widest range of applications. Dielectric ? Embedding, Encapsulating, Insulating, Patching, and Bonding of the greatest variety of electric/electronic components for exterior and interior exposure, corrosive, and other problem environments.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 100 %100 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D >= 80>= 80
Tensile Strength at Break 35.2 MPa5100 psi
Flexural Strength 57.2 MPa8300 psi
Flexural Modulus 1.45 GPa210 ksi
Compressive Strength 92.4 MPa13400 psi
Compressive Modulus 1.86 GPa270 ksi
Izod Impact, Notched 0.214 J/cm0.400 ft-lb/in
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 70.0 °C158 °FDeflection Temp at unknown load
 
Processing PropertiesMetricEnglishComments
Pot Life 12 - 14 min12 - 14 min
Shelf Life >= 12.0 Month>= 12.0 Month
 
Descriptive Properties
ColorLight Gray
Hardening Time (min)6-240depending on temp.
Viscositythixotropic, no-slump paste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hardwire 3x2-23-12 High Density Tape
Mid-Mountain Materials CERMEX® BK2200SW Low Biopersistence Thermal Insulation Blanket
Mid-Mountain Materials CERMEX® BK1800SW Low Biopersistence Thermal Insulation Blanket
Hexcel® HexWeb® CR III 1/16-5052-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb
Henkel Hysol PL 795 Film Adhesive

PABC832 / 107816

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.