MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aluminum Bronze, UNS C61300, Cold Finished
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Good to excellent corrosion resistance. Good hot and cold formability. Fair to poor machinability

Applications: nuts, bolts, stringers and threaded members, corrosion resistant vessels and tanks, structural components, machine parts, condenser tube and piping systems, marine protective sheathing and fasteners, munitions mixing troughs and blending chambers.

Properties typical for 13mm thick plate .

Key Words: CDA 613
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.89 g/cc0.285 lb/in³approximately 1.8% volume contraction on freezing
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell  49
@Load 3000 kg,
Temperature 538 °C
49
@Load 6610 lb,
Temperature 1000 °F
 83
@Load 3000 kg,
Temperature 427 °C
83
@Load 6610 lb,
Temperature 801 °F
 137
@Load 3000 kg,
Temperature 316 °C
137
@Load 6610 lb,
Temperature 601 °F
 144
@Load 3000 kg,
Temperature 204 °C
144
@Load 6610 lb,
Temperature 399 °F
 157
@Load 3000 kg,
Temperature 20.0 °C
157
@Load 6610 lb,
Temperature 68.0 °F
 162
@Load 3000 kg,
Temperature -29.0 °C
162
@Load 6610 lb,
Temperature -20.2 °F
 170
@Load 3000 kg,
Temperature -60.0 °C
170
@Load 6610 lb,
Temperature -76.0 °F
 186
@Load 3000 kg,
Temperature -182 °C
186
@Load 6610 lb,
Temperature -296 °F
Tensile Strength, Ultimate  88.0 MPa
@Temperature 538 °C
12800 psi
@Temperature 1000 °F
 170 MPa
@Temperature 427 °C
24700 psi
@Temperature 801 °F
 432 MPa
@Temperature 316 °C
62700 psi
@Temperature 601 °F
 532 MPa
@Temperature 204 °C
77200 psi
@Temperature 399 °F
 590 MPa
@Temperature 20.0 °C
85600 psi
@Temperature 68.0 °F
 606 MPa
@Temperature -29.0 °C
87900 psi
@Temperature -20.2 °F
 611 MPa
@Temperature -60.0 °C
88600 psi
@Temperature -76.0 °F
 718 MPa
@Temperature -182 °C
104000 psi
@Temperature -296 °F
Tensile Strength, Yield  71.0 MPa
@Strain 0.5 %,
Temperature 538 °C
10300 psi
@Strain 0.5 %,
Temperature 1000 °F
 105 MPa
@Strain 0.5 %,
Temperature 427 °C
15200 psi
@Strain 0.5 %,
Temperature 801 °F
 271 MPa
@Strain 0.5 %,
Temperature 316 °C
39300 psi
@Strain 0.5 %,
Temperature 601 °F
 298 MPa
@Strain 0.5 %,
Temperature 204 °C
43200 psi
@Strain 0.5 %,
Temperature 399 °F
 318 MPa
@Strain 0.5 %,
Temperature 20.0 °C
46100 psi
@Strain 0.5 %,
Temperature 68.0 °F
 335 MPa
@Strain 0.5 %,
Temperature -60.0 °C
48600 psi
@Strain 0.5 %,
Temperature -76.0 °F
 339 MPa
@Strain 0.5 %,
Temperature -29.0 °C
49200 psi
@Strain 0.5 %,
Temperature -20.2 °F
 397 MPa
@Strain 0.5 %,
Temperature -182 °C
57600 psi
@Strain 0.5 %,
Temperature -296 °F
Elongation at Break  22 %
@Temperature 316 °C
22 %
@Temperature 601 °F
 27 %
@Temperature 538 °C
27 %
@Temperature 1000 °F
 35 %
@Temperature 204 °C
35 %
@Temperature 399 °F
 42 %
@Temperature 20.0 °C
42 %
@Temperature 68.0 °F
 44 %
@Temperature -29.0 °C
44 %
@Temperature -20.2 °F
 45 %
@Temperature -60.0 °C
45 %
@Temperature -76.0 °F
 50 %
@Temperature -182 °C
50 %
@Temperature -296 °F
 52 %
@Temperature 427 °C
52 %
@Temperature 801 °F
Reduction of Area  24 %
@Temperature 316 °C
24 %
@Temperature 601 °F
 26 %
@Temperature 538 °C
26 %
@Temperature 1000 °F
 32 %
@Temperature 204 °C
32 %
@Temperature 399 °F
 41 %
@Temperature 427 °C
41 %
@Temperature 801 °F
 49 %
@Temperature -182 °C
49 %
@Temperature -296 °F
 55 %
@Temperature -60.0 °C
55 %
@Temperature -76.0 °F
 58 %
@Temperature -29.0 °C
58 %
@Temperature -20.2 °F
 59 %
@Temperature 20.0 °C
59 %
@Temperature 68.0 °F
Modulus of Elasticity 115 GPa16700 ksi
 45.0 GPa
@Temperature 538 °C
6530 ksi
@Temperature 1000 °F
 48.0 GPa
@Temperature 427 °C
6960 ksi
@Temperature 801 °F
 88.0 GPa
@Temperature 316 °C
12800 ksi
@Temperature 601 °F
 126 GPa
@Temperature 20.0 °C
18300 ksi
@Temperature 68.0 °F
 128 GPa
@Temperature 204 °C
18600 ksi
@Temperature 399 °F
 149 GPa
@Temperature -60.0 °C
21600 ksi
@Temperature -76.0 °F
 156 GPa
@Temperature -182 °C
22600 ksi
@Temperature -296 °F
 172 GPa
@Temperature -29.0 °C
24900 ksi
@Temperature -20.2 °F
Poissons Ratio 0.3120.312
Fatigue Strength 180 MPa
@# of Cycles 1.00e+8
26100 psi
@# of Cycles 1.00e+8
Reverse Bending; Temper Not Reported
Machinability 30 %30 %Based on 100% machinability for UNS C360000
Forgeability 50 %50 %
Shear Modulus 44.0 GPa6380 ksi
Izod Impact 54.0 - 66.0 J
@Temperature -30.0 - 150 °C
39.8 - 48.7 ft-lb
@Temperature -22.0 - 302 °F
Temper not specified
Charpy Impact  41.0 J
@Temperature 550 °C
30.2 ft-lb
@Temperature 1020 °F
V-notch
 58.0 J
@Temperature 425 °C
42.8 ft-lb
@Temperature 797 °F
V-notch
 85.0 J
@Temperature 320 °C
62.7 ft-lb
@Temperature 608 °F
V-notch
 90.0 J
@Temperature 200 °C
66.4 ft-lb
@Temperature 392 °F
V-notch
 95.0 J
@Temperature -175 °C
70.1 ft-lb
@Temperature -283 °F
V-notch
 104 J
@Temperature -50.0 °C
76.7 ft-lb
@Temperature -58.0 °F
V-notch
 106 J
@Temperature 0.000 °C
78.2 ft-lb
@Temperature 32.0 °F
V-notch
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000144 ohm-cm
@Temperature 20.0 °C
0.0000144 ohm-cm
@Temperature 68.0 °F
Magnetic Permeability 1.161.16
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.2 µm/m-°C
@Temperature 20.0 - 300 °C
9.00 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.375 J/g-°C0.0896 BTU/lb-°F
Thermal Conductivity 56.5 W/m-K
@Temperature 20.0 °C
392 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 1040 - 1045 °C1900 - 1913 °F
Solidus 1040 °C1900 °F
Liquidus 1045 °C1913 °F
Annealing Point 607.2 - 871 °C1125 - 1600 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 1010 °C1850 °FHot-Shortness Temperature
Annealing Temperature 600 - 875 °C1110 - 1610 °F
Hot-Working Temperature 800 - 925 °C1470 - 1700 °F
Recrystallization Temperature 785 - 870 °C1450 - 1600 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 6.0 - 7.5 %6.0 - 7.5 %
Copper, Cu 88.5 - 91.5 %88.5 - 91.5 %
Iron, Fe 2.0 - 3.0 %2.0 - 3.0 %
Lead, Pb <= 0.010 %<= 0.010 %
Manganese, Mn <= 0.10 %<= 0.10 %
Other, total <= 0.050 %<= 0.050 %
Tin, Sn 0.020 - 0.50 %0.020 - 0.50 %
Zinc, Zn <= 0.050 %<= 0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum Bronze, UNS C61300, Annealed
Aluminum bronze 5%, UNS C60800
Nickel Aluminum Bronze, UNS C63000, HR50 Temper
8% Aluminum Bronze, UNS C61000
Aluminum Bronze D, UNS C61400, Annealed Rod

MC61300b2 / 171635

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.