MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

8% Aluminum Bronze, UNS C61000
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Good to excellent corrosion resistance. Good hot and cold workability.

Applications: bolts, pump parts, shafts, tie rods, overlay on steel for wearing surfaces.

Properties typical for rod, 25mm in diameter.

Key Words: CDA 610
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.78 g/cc0.281 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 6060O60 temper
 8585H04 temper
Tensile Strength, Ultimate 480 MPa69600 psiO60 temper
 550 MPa79800 psiH04 temper
Tensile Strength, Yield 205 MPa29700 psiO60 temper
 380 MPa55100 psiH04 temper
Elongation at Break 25 %25 %in 50 mm, H04 temper
 65 %65 %in 50 mm, O60 temper
Modulus of Elasticity 117 GPa17000 ksi
Poissons Ratio 0.330.33Calculated
Machinability 20 %20 %UNS C36000 (free-cutting brass) = 100%
Forgeability 70 %70 %
Shear Modulus 44.0 GPa6380 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000115 ohm-cm
@Temperature 20.0 °C
0.0000115 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.9 µm/m-°C
@Temperature 20.0 - 300 °C
9.94 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.375 J/g-°C0.0896 BTU/lb-°F
Thermal Conductivity 69.0 W/m-K
@Temperature 20.0 °C
479 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point <= 1040 °C<= 1900 °F
Liquidus 1040 °C1900 °F
Annealing Point 593 - 677 °C1100 - 1250 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 600 - 675 °C1110 - 1250 °F
Hot-Working Temperature 760 - 875 °C1400 - 1610 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 6.0 - 8.5 %6.0 - 8.5 %
Copper, Cu 92 %92 %
Iron, Fe <= 0.50 %<= 0.50 %
Lead, Pb <= 0.020 %<= 0.020 %
Other, total <= 0.50 %<= 0.50 %
Silicon, Si <= 0.10 %<= 0.10 %
Zinc, Zn <= 0.20 %<= 0.20 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum Bronze, UNS C61300, Annealed
Nickel Aluminum Bronze, UNS C63000, HR50 Temper
Aluminum bronze 5%, UNS C60800
Aluminum Bronze D, UNS C61400, Annealed Rod
Aluminum Bronze, UNS C61300, Cold Finished

MC61000b1 / 11578

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.