System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Braskem UTEC® 5040 Ultra High Molecular Weight Polyethylene
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
Polyethylene (PE)
;
High Density (HDPE)
;
UHMW PE (Ultra High Molecular Weight PE)
Material Notes:
Applications which require high wear resistance - technical parts, RAM extruded and compression molded sheets, rods and profiles.
Information provided by Braskem.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
0.930
g/cc
0.930
g/cc
ASTM D792/ISO 1183
Bulk Density
0.450
g/cc
0.0163
lb/in³
ASTM D-1895
Particle Size
190
µm
190
µm
Average; D50; ASTM D1921
230
µm
230
µm
Average; D50; Laser scattering; ISO 13320-1
Viscosity Test
2400
cm³/g
24.0
dl/g
Intrinsic; ASTM D4020
Molecular Weight
6.00e+6
g/mol
6.00e+6
g/mol
Braskem
Mechanical Properties
Metric
English
Comments
Hardness, Shore D
64
64
ASTM D2240/ISO 868
Tensile Strength at Break
>=
30.0
MPa
>=
4350
psi
ASTM D638
Charpy Impact, Notched
>=
10.0
J/cm²
>=
47.6
ft-lb/in²
Determined with double-notched specimens; ISO 11542-2
Coefficient of Friction, Dynamic
0.090
0.090
ASTM D1894
Coefficient of Friction, Static
0.10
0.10
ASTM D-1894
Abrasion
82
82
ISO 15527 reference set as 100; Braskem (sand slurry)
Descriptive Properties
Elongation Stress
0.41 MPa
ISO 11542-2; (150/10)
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Braskem UTEC® 4040 Ultra High Molecular Weight Polyethylene
Braskem UTEC® 3040 Ultra High Molecular Weight Polyethylene
Braskem UTEC® 4041 Ultra High Molecular Weight Polyethylene
Braskem UTEC® 5041 Ultra High Molecular Weight Polyethylene
Braskem UTEC® 6541 Ultra High Molecular Weight Polyethylene
PBRAS771 / 109482
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.