MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Braskem UTEC® 5041 Ultra High Molecular Weight Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: Applications which require high wear resistance and the use of pigments and/or additives - technical parts, RAM extruded and compression molded sheets, rods and profiles.

Information provided by Braskem.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.930 g/cc0.930 g/ccASTM D792/ISO 1183
Bulk Density 0.450 g/cc0.0163 lb/in³ASTM D-1895
Particle Size 130 µm130 µmAverage; D50; ASTM D1921
 150 µm150 µmAverage; D50; Laser scattering; ISO 13320-1
Viscosity Test 2400 cm³/g24.0 dl/gIntrinsic; ASTM D4020
Molecular Weight 6.00e+6 g/mol6.00e+6 g/molBraskem
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6464ASTM D2240/ISO 868
Tensile Strength at Break >= 30.0 MPa>= 4350 psiASTM D638
Charpy Impact, Notched >= 10.0 J/cm²>= 47.6 ft-lb/in²Determined with double-notched specimens; ISO 11542-2
Coefficient of Friction, Dynamic 0.0900.090ASTM D1894
Coefficient of Friction, Static 0.100.10ASTM D-1894
Abrasion 8282ISO 15527 reference set as 100; Braskem (sand slurry)
 
Descriptive Properties
Elongation Stress0.41 MPaISO 11542-2; (150/10)

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem UTEC® 4040 Ultra High Molecular Weight Polyethylene
Braskem UTEC® 3040 Ultra High Molecular Weight Polyethylene
Braskem UTEC® 4041 Ultra High Molecular Weight Polyethylene
Braskem UTEC® 5040 Ultra High Molecular Weight Polyethylene
Titanium Grade 1

PBRAS772 / 109483

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.