MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Buckeye Polymers BP RPP 2009 GK BLK Polypropylene, 20% Glass Filled
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Glass Fiber Filler

Material Notes: Product Information: Our glass reinforced product lines exhibit increased tensile strength, stiffness, and heat deflection. Highly optimized glass reinforced PP resins have successfully replaced engineering thermoplastics in numerous applications.

    Product Features:
  • Good flexural strength
  • Appearance: Black

    Forms: Pellets

    Processing Method: Injection Moulding

    Information Provided by Buckeye Polymers, Inc.

Key Words: glass content 16-22%
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Carbon Black Loading 1.0 %1.0 %
Melt Flow 2.0 - 12 g/10 min2.0 - 12 g/10 minASTM D1238
Ash 16 - 22 %16 - 22 %ASTM D5630
 
Mechanical PropertiesMetricEnglishComments
Flexural Modulus >= 1.49461 GPa>= 216.775 ksiASTM D790

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical LUPOL GP-2201F General Purpose Polypropylene, 20% Glass Fiber Reinforced, Flame Retardant
LG Chemical LUPOL GP2150 PP+GF15%
E-Polymers TEKAFINĀ® PH50G2 20% Glass Fiber Reinforced High Strength Compounded-PP
Cossa Polimeri ESTAPROP H 0540 GFC Polypropylene, 20% Glass Filled
Cheng Yu Plastic PP237G2 Polypropylene, 20% Glass Fiber

PBUCK011 / 104479

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.