MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Overview of materials for AISI 6000 Series Steel
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 6000 Series Steel

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "AISI 6000 Series Steel". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.85 - 7.86 g/cc0.284 - 0.284 lb/in³Average value: 7.85 g/cc Grade Count:37
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 170 - 363170 - 363Average value: 281 Grade Count:37
Hardness, Knoop 219 - 392219 - 392Average value: 309 Grade Count:36
Hardness, Rockwell B 92.0 - 10092.0 - 100Average value: 98.0 Grade Count:36
Hardness, Rockwell C 13.0 - 40.013.0 - 40.0Average value: 28.8 Grade Count:36
Hardness, Vickers 207 - 384207 - 384Average value: 299 Grade Count:36
Tensile Strength, Ultimate 670 - 1240 MPa97200 - 180000 psiAverage value: 992 MPa Grade Count:34
Tensile Strength, Yield 415 - 1230 MPa60200 - 178000 psiAverage value: 824 MPa Grade Count:34
Elongation at Break 14.5 - 23.0 %14.5 - 23.0 %Average value: 18.2 % Grade Count:34
Modulus of Elasticity 205 - 207 GPa29700 - 30000 ksiAverage value: 205 GPa Grade Count:37
Bulk Modulus 160 GPa23200 ksiAverage value: 160 GPa Grade Count:36
Poissons Ratio 0.2900.290Average value: 0.290 Grade Count:36
Machinability 55.0 - 60.0 %55.0 - 60.0 %Average value: 55.3 % Grade Count:36
Shear Modulus 80.0 GPa11600 ksiAverage value: 80.0 GPa Grade Count:36
Izod Impact 27.0 - 35.0 J19.9 - 25.8 ft-lbAverage value: 31.0 J Grade Count:4
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000234 ohm-cm0.0000234 ohm-cmAverage value: 0.0000234 ohm-cm Grade Count:36
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 0.475 J/g-°C0.114 BTU/lb-°FAverage value: 0.475 J/g-°C Grade Count:36
Thermal Conductivity 46.6 W/m-K323 BTU-in/hr-ft²-°FAverage value: 46.6 W/m-K Grade Count:36
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.150 - 0.540 %0.150 - 0.540 %Average value: 0.487 % Grade Count:37
Chromium, Cr 0.400 - 1.20 %0.400 - 1.20 %Average value: 0.944 % Grade Count:37
Iron, Fe 96.9 - 98.8 %96.9 - 98.8 %Average value: 97.4 % Grade Count:37
Manganese, Mn 0.400 - 1.00 %0.400 - 1.00 %Average value: 0.789 % Grade Count:37
Phosphorus, P 0.0350 %0.0350 %Average value: 0.0350 % Grade Count:36
Silicon, Si 0.150 - 0.300 %0.150 - 0.300 %Average value: 0.227 % Grade Count:37
Sulfur, S 0.0400 %0.0400 %Average value: 0.0400 % Grade Count:36
Vanadium, V 0.100 - 0.150 %0.100 - 0.150 %Average value: 0.149 % Grade Count:37

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for AISI 4000 Series Steel
Overview of materials for AISI 5000 Series Steel
Overview of materials for AISI 9000 Series Steel
Overview of materials for AISI 8000 Series Steel
Overview of materials for Low Alloy Steel

M01002 / 81708

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.