MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow DOWLEX™ 2085G Polyethylene Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: DOWLEX™ 2085G is an ethylene-octene copolymer designed for general purpose thin gauge film applications. It is perfect for high strength consumer trash bags/liners. This product can be used in other applications that require toughness and also offer good melt strength for high throughput rates.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³ASTM D792
Thickness 20.3 microns0.800 mil
Melt Flow 0.85 g/10 min0.85 g/10 minASTM D1238
Antiblock Level 5000 ppm5000 ppm
Slip Level 900 ppm900 ppm
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 11.4 MPa1650 psiASTM D882
Film Tensile Strength at Yield, TD 10.51 MPa1525 psiASTM D882
Film Elongation at Break, MD 370 %370 %ASTM D882
Film Elongation at Break, TD 620 %620 %ASTM D882
Elmendorf Tear Strength MD 300 g300 gASTM D1922
Elmendorf Tear Strength TD 475 g475 gASTM D1922
Elmendorf Tear Strength, MD 14.8 g/micron375 g/milASTM D1922
Elmendorf Tear Strength, TD 23.376 g/micron593.75 g/milASTM D1922
Dart Drop Test 400 g0.882 lbMethod A; ASTM D1709
Film Tensile Strength at Break, MD 46.9 MPa6800 psiASTM D882
Film Tensile Strength at Break, TD 42.7 MPa6200 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 121 °C250 °FDow Method (DSC)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow DOWLEX™ 2045G Linear Low Density Polyethylene
Dow DOWLEX™ 2020G Linear Low Density Polyethylene
Dow DOWLEX™ 2056G Linear Low Density Polyethylene
Dow DOWLEX™ 2035 Linear Low Density Polyethylene, Cast Film Grade
Dow DOWLEX™ 2077G Linear Low Density Polyethylene

PDOW1317 / 30535

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.