MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Celanex® 3109HR PBT, 7.5% Glass Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled

Material Notes: Celanex 3109HR is a non-lubricated, 7.5% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties, and processability.
7.5% glass filled

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.35 g/cc1.35 g/ccASTM D792
Density 1.35 g/cc0.0488 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0060 - 0.010 cm/cm0.0060 - 0.010 in/inASTM D955
 0.0060 - 0.010 cm/cm0.0060 - 0.010 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.010 - 0.014 cm/cm0.010 - 0.014 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 66.9 MPa9700 psiASTM D638
 78.0 MPa11300 psi5mm/min; ISO 527-2/1A
Tensile Strength, Yield 79.3 MPa11500 psiASTM D638
Elongation at Break 8.0 %8.0 %5mm/min; ISO 527-2/1A
 8.5 %
@Temperature 22.8 °C
8.5 %
@Temperature 73.0 °F
ASTM D638
Tensile Modulus 3.10 GPa
@Temperature 22.8 °C
450 ksi
@Temperature 73.0 °F
ASTM D638
Flexural Strength 105 MPa15200 psiISO 178
 110 MPa16000 psiASTM D790
Flexural Modulus 3.55 GPa515 ksiISO 178
 3.45 GPa
@Temperature 22.8 °C
500 ksi
@Temperature 73.0 °F
ASTM D790
Izod Impact, Notched (ISO) 3.80 kJ/m²1.81 ft-lb/in²ISO 180/1A
Izod Impact, Unnotched (ISO) 23.0 kJ/m²10.9 ft-lb/in²ISO 180/1U
Charpy Impact Unnotched NBNBISO 179/1eU
 19.0 J/cm²
@Temperature -30.0 °C
90.4 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.600 J/cm²2.86 ft-lb/in²ISO 179/1eA
 0.550 J/cm²
@Temperature -30.0 °C
2.62 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmIEC 60093
 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmIEC 60093
Dielectric Constant  3.6
@Frequency 1e+6 Hz
3.6
@Frequency 1e+6 Hz
IEC 60250
 4.0
@Frequency 100 Hz
4.0
@Frequency 100 Hz
IEC 60250
Dielectric Strength 18.5 kV/mm470 kV/inshort term; ASTM D149
 23.0 kV/mm584 kV/inIEC 60243-1
Dissipation Factor  0.0013
@Frequency 100 Hz
0.0013
@Frequency 100 Hz
IEC 60250
 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
IEC 60250
Arc Resistance 130 sec130 secASTM D495
Comparative Tracking Index 250 V250 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
CTE, linear 130 µm/m-°C72.2 µin/in-°FISO 11359-2
Specific Heat Capacity 1.97 J/g-°C0.471 BTU/lb-°FInternal
Thermal Conductivity 0.131 W/m-K0.909 BTU-in/hr-ft²-°FInternal
Melting Point 225 °C437 °F10°C/min; ISO 11357-1,-2,-3
 225 °C437 °FASTM D3418
Transformation Temperature, Tg 60.0 °C140 °F10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 0.46 MPa (66 psi) 206 °C403 °FISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 143 °C289 °FISO 75-1, -2
Vicat Softening Point 185 °C365 °FB50 (50°C/h 50N); ISO 306
Oxygen Index 22 %22 %ISO 4589
 
Processing PropertiesMetricEnglishComments
Processing Temperature 20.0 - 50.0 °C68.0 - 122 °F
 65.0 - 93.0 °C149 - 199 °FCavity temperature
Feed Temperature 230 - 240 °C446 - 464 °F
Rear Barrel Temperature 230 - 240 °C446 - 464 °F
Middle Barrel Temperature 235 - 250 °C455 - 482 °F
Front Barrel Temperature 240 - 260 °C464 - 500 °F
Nozzle Temperature 250 - 260 °C482 - 500 °F
Zone 1 230 - 240 °C446 - 464 °F
Zone 2 235 - 250 °C455 - 482 °F
Zone 3 235 - 250 °C455 - 482 °F
Zone 4 240 - 260 °C464 - 500 °F
Die Temperature 250 - 260 °C482 - 500 °F
Melt Temperature 240 - 260 °C464 - 500 °F
 260 °C500 °FInjection molding; ISO 294
Mold Temperature 65.6 - 93.3 °C150 - 200 °F
 82.0 °C180 °FInjection molding; ISO 294
Injection Velocity 300 mm/sec11.8 in/secISO 294
Drying Temperature 120 - 130 °C248 - 266 °F
Dry Time 4.00 hour4.00 hour
Moisture Content 0.020 %0.020 %Necessary low maximum residual
Hold Pressure 48.0 MPa6960 psiISO 294
Back Pressure 0.000 - 0.345 MPa0.000 - 50.0 psi
Hot-Working Temperature 250 - 260 °C482 - 500 °F
 
Descriptive Properties
Injection moldingYes
Injection speedmedium-fast
Longer pre-drying times/storagelower the temperature to 100° C until processed.<= 60 h
Processing conditionsISO 7792-2
Processing NotesFast Injection Speed
 Medium Screw Speed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik Vestodur® X9400 10% Glass Reinforced PBT
Envalior Arnite® TV6 220 PBT-GF10
Celanese Vandar® 4632Z PBT, 15% Glass Reinforced
Celanese Impet® 610R Recycled PET, 13% Glass/Mineral Reinforced

PHCR035 / 158602

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.