MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik Vestodur® X9400 10% Glass Reinforced PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled

Material Notes: Description: VESTODUR X9400 is a 10 % glass fiber reinforced, polymer-modified polybutylene terephthalate compound. Moldings of this compound show decreased shrinkage. The compound is suitable for parts that are subjected to high mechanical or thermal loads. Compared with commonly used glass fiber reinforced PBT compounds with a similar stiffness parts of VESTODUR X9400 have in particular a high surface quality

Information provided by degussa.

Evonik Industries is the successor company to Degussa.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.35 g/cc0.0488 lb/in³ISO 1183
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm
@Thickness 2.00 mm
0.0020 - 0.0040 in/in
@Thickness 0.0787 in
sheet with film gate at rim, mold temperature 80°C
Linear Mold Shrinkage, Transverse 0.0030 - 0.0050 cm/cm0.0030 - 0.0050 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 90.0 MPa13100 psiISO 527-1/2
Elongation at Break 5.5 %5.5 %ISO 527-1/2
Elongation at Yield 4.0 %4.0 %ISO 527-1/2
Tensile Modulus 4.50 GPa653 ksiISO 527-1/-2
Charpy Impact Unnotched  4.50 J/cm²
@Temperature -30.0 °C
21.4 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 4.50 J/cm²
@Temperature 23.0 °C
21.4 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.500 J/cm²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.500 J/cm²
@Temperature 23.0 °C
2.38 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 200 °C392 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 110 °C230 °FISO 75-1/-2
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
IEC 60695

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Celanex® 3109HR PBT, 7.5% Glass Reinforced
Celanese Vandar® 4632Z PBT, 15% Glass Reinforced
Celanese Impet® 610R Recycled PET, 13% Glass/Mineral Reinforced
Envalior Arnite® TV6 220 PBT-GF10
Eurofoam Porocell POR 446 NDN NR-SBR Foam

PHUMA71 / 47585

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.