MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ExxonMobil Santoprene® 111-87 Thermoplastic Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range of injection molding applications. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding. It is polyolefin based and completely recyclable.

  • Recommended for applications requiring excellent flex fatigue resistance.
  • Excellent ozone resistance.
  • Designed for applications requiring high-flow materials.
  • Recommended for applications requiring superior part surface appearance.

Information provided by Advanced Elastomer Systems

Key Words: EU 2003/11/EC; RoHS Compliant; UL QMFZ2; UL QMFZ8
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.960 g/cc0.960 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8787.12 in; ASTM D2240
Tensile Strength at Break 8.736 MPa1267 psi257°F, 70 hr, in IRM 903 Oil; ASTM D471
 10.608 MPa1538.5 psiAir at 302°F, 168 hr; ASTM D573
 12.5 MPa1810 psiAcross Flow; ASTM D412
Tensile Strength, Ultimate 6.48 MPa940 psiAcross Flow; ASTM D412
Elongation at Break 290.7 %290.7 %257°F, 70 hr, in IRM 903 Oil; ASTM D471
 387.6 %387.6 %Air at 302°F, 168 hr; ASTM D573
 510 %510 %Across Flow; ASTM D412
Compression Set  32 %
@Temperature 70.0 °C,
Time 79200 sec
32 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395
 63 %
@Temperature 125 °C,
Time 252000 sec
63 %
@Temperature 257 °F,
Time 70.0 hour
ASTM D395
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.62.6ASTM D150
Dielectric Strength 31.5 kV/mm800 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 135 °C275 °F
Brittleness Temperature -60.0 °C-76.0 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Processing Temperature 175 - 230 °C347 - 446 °F
Rear Barrel Temperature 177 - 193 °C350 - 380 °F
Middle Barrel Temperature 179 - 199 °C355 - 390 °F
Front Barrel Temperature 179 - 204 °C355 - 400 °F
Nozzle Temperature 191 - 229 °C375 - 445 °F
Melt Temperature 193 - 241 °C380 - 465 °FProcessing
Mold Temperature 10.0 - 51.7 °C50.0 - 125 °FProcessing
Drying Temperature 82.2 °C180 °F
Dry Time 3 hour3 hour
Moisture Content 0.080 %0.080 %
Back Pressure 0.345 - 0.689 MPa50.0 - 100 psiProcessing
Clamp Pressure 41.4 - 68.9 MPa6000 - 10000 psi
Vent Depth 0.00254 cm0.00100 in
Cushion 0.317 - 0.635 cm0.125 - 0.250 in
Screw Speed 100 - 200 rpm100 - 200 rpm
 
Descriptive Properties
Change in Mass in IRM 903 Oil at 257°F for 70 hr84
ColorBlack
FormPellets
Injection RateFast
Maximum Regrind %20
Screw Compression Ratio2:1 - 2.5:1
Screw L/D Ratio16:1 - 20:1

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Advanced Elastomer Systems Santoprene® 281-87 Thermoplastic Rubber
ExxonMobil Santoprene® 121-87 Thermoplastic Elastomer
ExxonMobil Santoprene® 101-87 Thermoplastic Elastomer
ExxonMobil Geolast® 701-80W183 Thermoplastic Elastomer
ExxonMobil Santoprene® 171-73 Thermoplastic Elastomer

PADVA054 / 22744

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.