MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Advanced Elastomer Systems Santoprene® 281-87 Thermoplastic Rubber  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, blow molding or other melt processing techniques. Drug Master File has been established at US FDA National Center for drugs and biologics.

Key Features: MEM elution cytotoxicity to L-929 mouse fibroblast cells, 72 hr. exposure to rubber extract; NAmSA, MT023-100 test method; test unit, % cell lysis; typical value 0; USP physiochemical test for elastomer closures, heavy metals such as lead; NAmSA, CP020-004 test method; Test unit, ppm; typical value <1

Additional processing comments: This thermoplastic rubber is a shear-dependent material that can be processed on conventional thermoplastic equipment for injection molding, extrusion, or blow molding. For extrusion, a general purpose screw with a compression ratio of 2.5 to 3.0 is recommended. Material can be recycled. SANTOPRENE rubber is incompatible with acetal and PVC.

Values below are for injection molded plaques, side gated, 82.6 mm x 117.5 mm x 3.0 mm. Tensile properties measured across flow. Data provided by Advanced Elastomer Systems.

Advanced Elastomer Systems is now a part of ExxonMobil. This grade was removed from the Advanced Elastomers Systems standard product line before the ExxonMobil acquisiton.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.960 g/cc0.0347 lb/in³TPE-0105 (ASTM D792)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 87875 Second; TPE-0169 (ASTM D 2240)
Tensile Strength, Ultimate 15.9 MPa2310 psiTPE-0153 (ASTM D 412)
Elongation at Break 530 %530 %TPE-0153 (ASTM D 412)
100% Modulus 7.00 MPa
@Strain 100 %
1020 psi
@Strain 100 %
TPE-0153 (ASTM D 412)
Tear Strength 49.0 kN/m280 pli49 kN/m at 23°C. Value at 100°C is 23 kN/m. TPE-0056 (ASTM D 624)
Compression Set 45 %
@Temperature 100 °C
45 %
@Temperature 212 °F
168 hrs.; TPE-0016 (ASTM D 412)
 29 %
@Temperature 23.0 °C,
Time 605000 sec
29 %
@Temperature 73.4 °F,
Time 168 hour
TPE-0016 (ASTM D 412)
Tensile Set 33 %33 %23°C, 168 hrs.; TPE-0053 (ASTM D 412)
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -60.0 °C<= -76.0 °FTPE-0089 (ASTM D 746)
 
Processing PropertiesMetricEnglishComments
Processing Temperature 177 - 232 °C351 - 450 °F
Drying Temperature 82.0 °C180 °FDesiccant drying for 3 hours recommended
Dry Time 3 hour3 hour
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 121-87 Thermoplastic Elastomer
ExxonMobil Santoprene® 111-87 Thermoplastic Elastomer
ExxonMobil Santoprene® 101-87 Thermoplastic Elastomer
Advanced Elastomer Systems Santoprene® 281-45 Thermoplastic Rubber
Advanced Elastomer Systems Santoprene® 181-55 Thermoplastic Rubber

PADV96 / 22686

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.