MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Master Bond Supreme 11LP Epoxy Resists Impact and Thermal Shock
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: This two component adhesive system is formulated to cure at room temperature or more rapidly at elevated temperatures, with a mix ratio (part A/part B: 100/100). Master Bond Polymer Adhesive SUPREME 11LP produces good performance bonds with both high shear and high peel strengths for service in the wide temperature range of below -100°F to over 300°F. It offers resistance to impact, thermal shock, vibration and stress fatigue cracking while maintaining the moisture, creep, corrosion and thermal resistance typical of epoxy resin adhesives. Master Bond Polymer Adhesive SUPREME 11LP is easily mixed and can be applied without sagging or dripping even on vertical surfaces. It is 100% reactive and does not contain any diluents or solvents. Master Bond Polymer System SUPREME 11LP produces durable, high strength, exceptionally tough bonds which are resistant to severe thermal cycling and many chemicals including water, oil, fuels and some organic solvents even upon prolonged exposures. Tensile shear strengths in excess of 1600 psi and T-peel strengths of 25 pli are readily obtained. Adhesion to metals, glass, ceramics, wood, vulcanized rubbers and many plastics is excellent. The hardened adhesive is a good electrical insulator. Color of part A is gray, part B is amber. SUPREME 11LP offers the convenience of a temperature cure with a favorable performance profile for use in even the most difficult applications in the aerospace, electronic, electrical, computer, construction, appliance, automotive and chemical industries.

Product Advantages:

  • Convenient mixing; non-critical mixing ratio (part A/part B: 100/100), by weight or volume.
  • Surface cleanliness not critical for good bonding in many cases but recommended for optimum strength.
  • Easy application; contact pressure only required for cure; adhesive spreads evenly and smoothly; no drip application feature.
  • Versatile cure schedules; ambient temperature cure or faster elevated temperature cures as required.
  • High shear and peel bonding strength to similar and dissimilar substrates over the remarkably wide temperature range of below -100°F to +300°F.
  • Good electrical insulating properties and chemical resistance.
  • Superior thermal shock, impact and stress cracking fatigue resistance.
  • Excellent long term durability.

Information provided by MasterBond®

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Viscosity 99000 - 121000 cP99000 - 121000 cPPart B
 108000 - 121200 cP108000 - 121200 cPPart A
 
Mechanical PropertiesMetricEnglishComments
Shear Strength >= 11.0 MPa>= 1600 psiTensile, Al to Al
Peel Strength 4.38 kN/m25.0 pliT-peel, Al to Al
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 149 °C300 °F
Minimum Service Temperature, Air -73.3 °C-100 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 900 - 1200 min
@Temperature 23.9 °C
15.0 - 20.0 hour
@Temperature 75.0 °F
85% of max strength
Pot Life 50 - 60 min50 - 60 min1 quart mass
 60 - 70 min60 - 70 min200 gram mass
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
Mixing Ratio (A to B)100/100

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond Supreme 11AOHTLO Epoxy Passes NASA Low Outgassing Tests
Master Bond Supreme 11HTLP One Component Epoxy
Master Bond Supreme 11HT-LO Adhesive and Sealant Serviceable to +400°F
Master Bond Supreme 11HT High Temperature Resistant Two Component Epoxy System
Master Bond Supreme 11AOHT Thermally Conductive, Heat Resistant Epoxy System

PMASTB353 / 149600

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.