MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Master Bond Supreme 11AOHTLO Epoxy Passes NASA Low Outgassing Tests
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: Master Bond Supreme 11AOHTLO is a two component epoxy resin system for high performance bonding and sealing. Although, it is formulated to cure at room temperature, the best cure schedule to attain optimal properties, including NASA low outgassing, is overnight at room temperature followed by a few hours at 150-200°F. It has a convenient one to one mix ratio by weight or volume. Its most outstanding features include high thermal conductivity, excellent electrical insulation properties and temperature resistance up to 400°F. Supreme 11AOHTL O is a “toughened” system which enables it to withstand rigorous thermal cycling and makes it well suited for bonding dissimilar substrates. It has excellent adhesion to most metals, ceramics, and glass as well as many rubbers and plastics. Its chemical resistance profile includes water, oil and fuels. Both Parts A and B are colored off-white. Master Bond Supreme 11AOHTLO is widely used in electronic, electro-optic, aerospace and vacuum applications where high strength, excellent thermal transfer properties, and high temperature resistance are required.

Product Advantages:

  • Convenient one to one mix ratio by weight or volume.
  • Versatile cure schedules: ambient or, for optimal properties, ambient combined with heat.
  • Excellent bond strength to a wide variety of substrates.
  • Toughened system, can withstand rigorous thermal cycling.
  • High thermal conductivity with exceptional electrical insulation properties.
  • Thermally stable up to 400°F with good thermal cycling properties.
  • Exceptionally good dimensional stability.
  • Passes NASA low outgassing.

Information provided by MasterBond®

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Viscosity 200000 - 300000 cP200000 - 300000 cPPart A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D >= 85>= 85
Tensile Modulus >= 3.10 GPa>= 450 ksi
Shear Strength >= 22.1 MPa>= 3200 psiBond, Al to Al
Peel Strength 2.63 kN/m15.0 pliT-peel, Al to Al
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cm
Dielectric Strength >= 15.7 kV/mm
@Thickness 3.17 mm
>= 400 kV/in
@Thickness 0.125 in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 35.0 - 40.0 µm/m-°C19.4 - 22.2 µin/in-°F
Thermal Conductivity 1.30 - 1.44 W/m-K9.00 - 10.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C400 °F
Minimum Service Temperature, Air -73.3 °C-100 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 60.0 - 120 min1.00 - 2.00 hourOptimum cure schedule, overnight at 75°F plus 150-200°F
 60.0 - 120 min
@Temperature 93.3 °C
1.00 - 2.00 hour
@Temperature 200 °F
 1440 - 2160 min
@Temperature 23.9 °C
24.0 - 36.0 hour
@Temperature 75.0 °F
Pot Life 15 - 25 min15 - 25 min100 gram mass
Shelf Life 6.00 Month
@Temperature 23.9 °C
6.00 Month
@Temperature 75.0 °F
in original unopened containers
 
Descriptive Properties
Mixing Ratio (A to B)1:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond EP17HT One component epoxy system for bonding, sealing, coating and casting
Master Bond Supreme 11LP Epoxy Resists Impact and Thermal Shock
Master Bond EP112LS Two part, heat curing epoxy for potting, encapsulation, coating, sealing and impregnation
Aremco Aremco-Bond™ 568 High Performance Epoxide
Master Bond Supreme 11AOHT Thermally Conductive, Heat Resistant Epoxy System

PMASTB351 / 149598

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.