MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco Aremco-Bond™ 568 High Performance Epoxide
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: Aluminum-Filled, 1:1, Good Bond Strength and High Thermal Conductivity.

Vendors: Aremco’s High Performance Epoxies provide a wide range of solutions for bonding ceramics, composites, glass, metals, plastics, and other materials. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.850 g/cc0.850 g/cc
Particle Size <= 20 µm<= 20 µm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7575
Flexural Strength 78.6 MPa11400 psiASTM D790
Shear Strength 17.2 MPa2500 psiASTM D1002-94
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1e+051e+05
Dielectric Strength 3.15 kV/mm80.0 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 59.4 µm/m-°C
@Temperature 20.0 °C
33.0 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 1.30 W/m-K9.00 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C400 °F
Minimum Service Temperature, Air -65.0 °C-85.0 °F
Shrinkage 0.20 %0.20 %Cure Shrinkage
 
Processing PropertiesMetricEnglishComments
Cure Time  120 min
@Temperature 93.3 °C
2.00 hour
@Temperature 200 °F
Recommended Cure
 1440 - 2880 min
@Temperature 23.0 °C
24.0 - 48.0 hour
@Temperature 73.4 °F
Alternate Cure
Pot Life 240 min
@Temperature 25.0 °C
240 min
@Temperature 77.0 °F
100 gm mass
 
Descriptive Properties
Chemical ResistanceExcellent
ColorGray
Mix Ratio by Weight1:1resin:hardener
Mixed ViscosityPaste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond Supreme 11LP Epoxy Resists Impact and Thermal Shock
Master Bond Supreme 11HTLP One Component Epoxy
Master Bond Supreme 11HT-LO Adhesive and Sealant Serviceable to +400°F
Master Bond Supreme 11HT High Temperature Resistant Two Component Epoxy System
Master Bond Supreme 11AOHTLO Epoxy Passes NASA Low Outgassing Tests

PAREM03 / 24267

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.